Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.251 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.155 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoPO4 + LiPO3 |
Band Gap1.228 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 127.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 80.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 242.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 205.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 240.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 297.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 137.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 225.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 205.8 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 112.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 255.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 130.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 212.6 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 242.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 340.2 |
Te2W (mp-22693) | <1 0 1> | <0 1 0> | 212.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 340.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 340.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 261.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 175.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 242.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 240.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 255.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 340.2 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 297.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 274.4 |
GaSe (mp-1943) | <0 0 1> | <1 1 -1> | 240.8 |
Al (mp-134) | <1 0 0> | <1 1 1> | 180.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 255.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 137.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 170.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 225.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 212.6 |
BN (mp-984) | <1 0 1> | <0 1 1> | 80.7 |
TeO2 (mp-2125) | <0 1 1> | <1 0 -1> | 225.3 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 212.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 -1> | 120.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 212.6 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 212.6 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 255.1 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 127.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 161.4 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 175.5 |
CdTe (mp-406) | <1 1 1> | <1 1 -1> | 240.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 255.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 297.6 |
C (mp-66) | <1 1 0> | <0 1 1> | 161.4 |
C (mp-66) | <1 1 1> | <0 1 0> | 340.2 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 242.1 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 242.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2As2O7 (mp-779594) | 0.4471 | 0.000 | 3 |
MnPO4 (mp-540022) | 0.6031 | 0.318 | 3 |
Zn2P2O7 (mp-559319) | 0.4842 | 0.000 | 3 |
Li2S2O7 (mp-1020013) | 0.4733 | 0.000 | 3 |
CuMoO4 (mvc-10504) | 0.6001 | 0.083 | 3 |
LiFeP2O7 (mp-762468) | 0.2430 | 0.254 | 4 |
LiNiP2O7 (mp-705295) | 0.3471 | 0.100 | 4 |
LiCrP2O7 (mp-705361) | 0.2580 | 0.185 | 4 |
LiFeP2O7 (mp-695816) | 0.1852 | 0.058 | 4 |
LiMnP2O7 (mp-697744) | 0.2173 | 0.212 | 4 |
CeSe2 (mp-1080324) | 0.7212 | 0.467 | 2 |
BaZn2As3HO11 (mp-758313) | 0.4912 | 0.007 | 5 |
Na2Li2V3P2O13 (mp-853239) | 0.7048 | 0.061 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.5863 eV |
Corrected Energy-315.5843 eV
Uncorrected energy = -289.7963 eV
Composition-based energy adjustment (-0.687 eV/atom x 28.0 atoms) = -19.2360 eV
Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV
Corrected energy = -315.5843 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)