Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.266 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCo(PO3)3 + CoPO4 + LiPO3 + O2 |
Band Gap0.001 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 0 1> | 195.3 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 132.7 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 266.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 293.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 241.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 195.3 |
Ag (mp-124) | <1 1 0> | <1 -1 0> | 265.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 246.0 |
Mg (mp-153) | <1 0 1> | <1 -1 0> | 132.7 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 241.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 293.0 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 195.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 195.3 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 293.0 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 -1> | 225.9 |
MgF2 (mp-1249) | <0 0 1> | <1 0 1> | 177.7 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 195.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 -1> | 266.4 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 293.0 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 246.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 293.0 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 293.0 |
TiO2 (mp-390) | <1 1 1> | <1 0 -1> | 266.4 |
ZnO (mp-2133) | <1 1 0> | <1 0 0> | 123.0 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 293.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4674 | 0.023 | 3 |
Co5(P3O11)2 (mp-31617) | 0.4235 | 0.034 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.4290 | 0.082 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4596 | 0.028 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4623 | 0.038 | 3 |
Li6V5(P2O7)4 (mp-765903) | 0.4178 | 0.051 | 4 |
LiVP2O7 (mp-705056) | 0.3744 | 0.032 | 4 |
LiFeP2O7 (mp-31827) | 0.4019 | 0.039 | 4 |
LiCoP2O7 (mp-585190) | 0.3813 | 0.055 | 4 |
LiMnP2O7 (mp-31971) | 0.3925 | 0.021 | 4 |
Cr19O48 (mp-850874) | 0.6887 | 0.097 | 2 |
LiMnV(P2O7)2 (mp-764615) | 0.3303 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764488) | 0.3252 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764481) | 0.3272 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764480) | 0.3273 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764622) | 0.3292 | 0.005 | 5 |
KLiMnP3HO10 (mp-764313) | 0.7313 | 0.046 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6257 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5868 | 0.330 | 6 |
CsAlBP2HO9 (mp-542129) | 0.7125 | 0.000 | 6 |
RbAlBP2HO9 (mp-542130) | 0.7341 | 0.000 | 6 |
K2NaCa2TiSi7HO20 (mp-720410) | 0.7388 | 0.000 | 7 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5439 | 0.002 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7286 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.6969 eV |
Corrected Energy-632.1246 eV
-632.1246 eV = -575.9304 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction) - 16.8660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)