Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.188 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.258 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeP2O7 + FePO4 + LiFe(PO3)4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP421c [114] |
HallP 4 2n |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 125.5 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 125.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 177.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 251.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 266.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.5 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 266.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 266.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 266.3 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 266.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 88.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 266.3 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 266.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 266.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 177.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 194.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 266.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 266.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 194.5 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 266.3 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 125.5 |
Au (mp-81) | <1 1 0> | <1 0 0> | 266.3 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 88.8 |
C (mp-48) | <1 0 0> | <1 1 0> | 251.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 251.1 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 266.3 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 266.3 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 251.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 194.5 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 266.3 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 194.5 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 266.3 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 194.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu3(P2O7)2 (mp-673105) | 0.7371 | 0.000 | 3 |
V3(P2O7)2 (mp-32416) | 0.7442 | 0.033 | 3 |
Mn3(P2O7)2 (mp-694554) | 0.7069 | 0.162 | 3 |
P4W3O14 (mvc-1031) | 0.6432 | 0.315 | 3 |
Fe3(P2O7)2 (mp-540486) | 0.7360 | 0.327 | 3 |
Li3V4P9O32 (mp-705002) | 0.1702 | 0.042 | 4 |
Li3Mo4P9O32 (mp-705341) | 0.1902 | 0.027 | 4 |
Li7Cr4P9O32 (mp-504389) | 0.4902 | 0.016 | 4 |
Li7Fe4P9O32 (mp-540520) | 0.4873 | 0.022 | 4 |
Li3Cr4P9O32 (mp-705371) | 0.1411 | 0.044 | 4 |
Ca10Mg7Al6Si17O60 (mp-677026) | 0.5778 | 0.017 | 5 |
Na2AlB(As2O7)2 (mp-556195) | 0.6197 | 0.004 | 5 |
Ca6Mg5Al2Si11O36 (mp-699405) | 0.5837 | 0.017 | 5 |
NaCaFe2(SiO3)4 (mvc-16542) | 0.6236 | 0.006 | 5 |
Ca2MgAl2(SiO4)3 (mp-677029) | 0.6156 | 0.019 | 5 |
Na2Ca6Mg7Fe(SiO3)16 (mp-745155) | 0.6135 | 0.031 | 6 |
NaCa3AlFe3(SiO3)8 (mp-743726) | 0.6115 | 0.158 | 6 |
NaCa5ScZn5(SiO3)12 (mp-705485) | 0.6000 | 0.036 | 6 |
KCa5Mg5Al(SiO3)12 (mp-534793) | 0.5990 | 0.033 | 6 |
NaCa9ScZn9(SiO3)20 (mp-720704) | 0.5925 | 0.038 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.6309 eV |
Corrected Energy-703.3755 eV
-703.3755 eV = -636.5649 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)