Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.171 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.305 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2FeP2HO8 |
Band Gap2.147 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 187.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 284.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 203.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 325.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 325.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 285.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 284.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 216.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 297.7 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 216.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 331.8 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 187.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 163.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 94.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 189.6 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 305.8 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 254.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 203.7 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 203.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 142.2 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 216.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 59.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 203.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 297.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 237.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 250.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 94.8 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 326.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 203.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 142.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 189.6 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 250.0 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 152.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 305.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 237.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 216.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 178.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 285.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 331.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 237.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 51.0 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 152.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 187.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 331.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 178.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 312.5 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 203.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 238.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 144.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.77372 | -2.08312 | 1.02581 | 0.00000 | 0.44534 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.63615 | 0.00000 | -0.59519 |
0.90211 | -1.48241 | -0.14095 | 0.00000 | 0.70922 | 0.00000 |
Piezoelectric Modulus ‖eij‖max3.00588 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.16 | 0.00 | 0.02 |
0.00 | 3.01 | 0.00 |
0.02 | 0.00 | 3.26 |
Dielectric Tensor εij (total) |
||
---|---|---|
15.91 | 0.00 | 5.04 |
0.00 | 8.70 | 0.00 |
5.04 | 0.00 | 11.45 |
Polycrystalline dielectric constant
εpoly∞
3.15
|
Polycrystalline dielectric constant
εpoly
12.02
|
Refractive Index n1.77 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-689981) | 0.6303 | 0.093 | 3 |
Sn8P2O13 (mp-767039) | 0.6376 | 0.025 | 3 |
V2Bi4O11 (mp-698685) | 0.6381 | 0.051 | 3 |
MoPb5O8 (mp-652366) | 0.6423 | 0.012 | 3 |
V2Bi4O11 (mp-690568) | 0.6460 | 0.074 | 3 |
Li3Bi(PO4)2 (mp-778460) | 0.6639 | 0.056 | 4 |
Cs2Si(HO2)2 (mp-995230) | 0.6478 | 0.061 | 4 |
VAs2H4O9 (mp-735567) | 0.6380 | 0.002 | 4 |
LiSb3(PO5)2 (mp-758492) | 0.6039 | 0.065 | 4 |
LiSnPO4 (mp-757042) | 0.6777 | 0.062 | 4 |
BaVCdP2O9 (mp-699566) | 0.6882 | 0.006 | 5 |
Rb2Cu3H2S3O14 (mp-697969) | 0.5387 | 0.250 | 5 |
LiFePH2O5 (mp-780200) | 0.6633 | 0.332 | 5 |
AgH2SNO3 (mp-697268) | 0.6593 | 0.062 | 5 |
Na2Al2Si3(HO3)4 (mp-510599) | 0.6688 | 0.565 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P H O |
Final Energy/Atom-6.2848 eV |
Corrected Energy-192.6759 eV
-192.6759 eV = -175.9733 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)