Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.744 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.327 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaAlSiO4 + CaCO3 |
Band Gap1.148 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63 [173] |
HallP 6c |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 144.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 124.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 124.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 216.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 144.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 249.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 72.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 216.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 72.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 288.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 136.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 288.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 136.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 249.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 288.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 288.2 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 72.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 72.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 216.1 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 288.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 136.5 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 124.8 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 216.1 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 154.3 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 216.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 288.2 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 72.0 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 124.8 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 216.1 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 288.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 72.0 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 72.0 |
Au (mp-81) | <1 1 0> | <1 0 0> | 72.0 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 154.3 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 216.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 216.1 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 154.3 |
C (mp-48) | <1 0 0> | <1 0 0> | 288.2 |
C (mp-48) | <1 1 0> | <1 0 0> | 288.2 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 288.2 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 216.1 |
ZnO (mp-2133) | <1 1 0> | <1 0 0> | 216.1 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 0> | 288.2 |
GaSb (mp-1156) | <1 0 0> | <1 0 1> | 154.3 |
SrTiO3 (mp-4651) | <0 0 1> | <1 1 0> | 124.8 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 144.1 |
ZnTe (mp-2176) | <1 0 0> | <1 0 1> | 154.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 288.2 |
SiC (mp-8062) | <1 0 0> | <1 0 1> | 154.3 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 216.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2V2O5 (mp-779376) | 0.6797 | 0.191 | 3 |
Cu2PO4 (mp-17281) | 0.6671 | 0.002 | 3 |
Li2Cr2O7 (mp-772666) | 0.7229 | 0.079 | 3 |
Ag6Ge2O7 (mp-15487) | 0.7494 | 0.022 | 3 |
SiAg5ClO4 (mp-647305) | 0.5921 | 0.027 | 4 |
LiSnPO4 (mp-757901) | 0.6692 | 0.067 | 4 |
CuSi(HO2)2 (mp-23731) | 0.6893 | 0.067 | 4 |
LiFe2P2HO8 (mp-763773) | 0.6766 | 0.024 | 5 |
KLiH2WO5 (mp-764147) | 0.6962 | 0.005 | 5 |
NaZnSiHO4 (mp-699219) | 0.5121 | 0.000 | 5 |
LiCrPH2O5 (mp-781961) | 0.6701 | 0.253 | 5 |
MnZn2Si(HO3)2 (mp-745154) | 0.5695 | 0.132 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ca_sv Al Si C O |
Final Energy/Atom-6.8353 eV |
Corrected Energy-376.5063 eV
-376.5063 eV = -355.4376 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)