Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.747 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAl2NiO4 |
Band Gap3.075 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 287.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 230.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 230.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 139.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 172.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 154.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 135.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 230.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 139.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 287.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 57.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 57.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 115.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 287.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 57.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 139.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 172.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 57.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 172.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 115.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 230.0 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 154.9 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 154.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 115.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 172.5 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 287.5 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 57.5 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 139.8 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 139.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 115.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 287.5 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 154.9 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 172.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 135.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 287.5 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 287.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 115.0 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 172.5 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 57.5 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 1> | 154.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 230.0 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 135.9 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 57.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 172.5 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 172.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2NiO4 (mp-699371) | 0.0732 | 0.005 | 3 |
Al2NiO4 (mp-705593) | 0.0196 | 0.012 | 3 |
Al2NiO4 (mp-705610) | 0.0171 | 0.009 | 3 |
Al2NiO4 (mvc-16266) | 0.0750 | 0.006 | 3 |
Al2NiO4 (mp-34234) | 0.0714 | 0.006 | 3 |
Li5Mn2Fe17O32 (mp-777733) | 0.1063 | 0.070 | 4 |
Li5Fe7O3F13 (mp-851009) | 0.1418 | 0.053 | 4 |
Li3Fe3OF7 (mp-764593) | 0.1559 | 0.045 | 4 |
Li3Zn(Fe5O8)4 (mp-771780) | 0.1134 | 0.067 | 4 |
Li5Co7O3F13 (mp-849472) | 0.1410 | 0.053 | 4 |
Fe3O4 (mp-715491) | 0.1898 | 0.015 | 2 |
Fe3O4 (mp-542433) | 0.2131 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.1671 | 0.057 | 2 |
Fe3O4 (mp-31770) | 0.2082 | 0.015 | 2 |
Fe3O4 (mp-716052) | 0.2235 | 0.073 | 2 |
Li4Fe3Cu3(SbO8)2 (mp-764385) | 0.2246 | 0.034 | 5 |
Li4Cr3Ni3(TeO8)2 (mp-761407) | 0.2073 | 0.007 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.2186 | 0.009 | 5 |
TaTi9Al3Zn23O48 (mp-686614) | 0.2190 | 0.054 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.1923 | 0.053 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6784 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6642 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6735 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6759 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6783 | 0.661 | 6 |
Explore more synthesis descriptions for materials of composition Al2NiO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Al Ni_pv O |
Final Energy/Atom-6.7602 eV |
Corrected Energy-522.9462 eV
-522.9462 eV = -473.2146 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction) - 21.6400 eV (MP Advanced Correction)
|