Final Magnetic Moment0.500 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.222 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.087 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe4P3(HO5)3 + FeHO2 + Li3PO4 + H2O |
Band Gap2.327 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 288.9 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 273.9 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 308.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 325.0 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 278.4 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 296.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 273.9 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 219.1 |
GaN (mp-804) | <1 1 1> | <1 -1 0> | 150.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 152.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 252.8 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 226.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 252.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 250.5 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 273.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 219.1 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 273.9 |
InAs (mp-20305) | <1 1 1> | <1 -1 1> | 250.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 296.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 296.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 231.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 308.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 229.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 361.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 361.1 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 231.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 180.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 229.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 273.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 229.0 |
YVO4 (mp-19133) | <1 1 1> | <1 1 1> | 250.5 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 273.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 252.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 216.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 273.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 325.0 |
GaSe (mp-1943) | <1 0 1> | <1 1 -1> | 208.5 |
Al (mp-134) | <1 1 0> | <0 1 1> | 296.9 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 308.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 54.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 273.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 180.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 252.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 219.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 -1 -1> | 250.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 219.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 296.9 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 325.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 361.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 216.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4P2O9 (mp-637226) | 0.6196 | 0.391 | 3 |
Mn4P2O9 (mp-770499) | 0.6008 | 0.015 | 3 |
Cr4P2O9 (mp-773396) | 0.6493 | 0.230 | 3 |
Ni4P2O9 (mp-771899) | 0.6667 | 0.037 | 3 |
Na2W2O7 (mp-25800) | 0.7234 | 0.021 | 3 |
Li3Bi(PO4)2 (mp-759624) | 0.5872 | 0.073 | 4 |
Mg2PHO5 (mp-23740) | 0.4978 | 0.000 | 4 |
Na6Mg(SO4)4 (mp-558427) | 0.5426 | 0.000 | 4 |
Li3Sn3(PO4)4 (mp-757551) | 0.5903 | 0.059 | 4 |
Li3V(PO4)2 (mp-540344) | 0.5901 | 0.057 | 4 |
LiVPHO5 (mp-767213) | 0.2511 | 0.000 | 5 |
LiCrPHO5 (mp-765883) | 0.2511 | 0.000 | 5 |
LiFePHO5 (mp-771864) | 0.2438 | 0.295 | 5 |
LiCoPHO5 (mp-770053) | 0.2648 | 0.025 | 5 |
LiAlPHO5 (mp-644409) | 0.2799 | 0.001 | 5 |
Li2VCrP2(HO5)2 (mp-765065) | 0.2361 | 0.113 | 6 |
Li2VFeP2(HO5)2 (mp-765061) | 0.2537 | 0.072 | 6 |
Li2VCrP2(HO5)2 (mp-767007) | 0.2537 | 0.048 | 6 |
Li2VCrP2(HO5)2 (mp-763879) | 0.2565 | 0.046 | 6 |
Li2VCrP2(HO5)2 (mp-765059) | 0.2501 | 0.095 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P H O |
Final Energy/Atom-6.3919 eV |
Corrected Energy-255.0858 eV
-255.0858 eV = -230.1080 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)