Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.048 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.642 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaH2N + H3N + AlN |
Band Gap0.733 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BN (mp-984) | <0 0 1> | <0 0 1> | 174.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 58.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 174.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 232.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 207.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 232.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 171.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 245.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 290.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 245.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 174.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 245.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 245.0 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 245.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 257.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.1 |
Al (mp-134) | <1 0 0> | <0 1 0> | 257.3 |
Al (mp-134) | <1 1 0> | <0 1 0> | 257.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 290.1 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 263.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 245.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 257.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 232.1 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 222.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 257.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 263.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 257.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 174.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 245.0 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 290.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 257.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 257.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 257.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 232.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 245.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 232.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 245.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 163.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 257.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 245.0 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 111.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 232.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 257.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 163.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 232.1 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 290.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 257.3 |
C (mp-66) | <1 0 0> | <0 1 0> | 257.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H5NO (mp-625924) | 0.5606 | 0.004 | 3 |
Si2H6Se (mp-29310) | 0.5937 | 0.000 | 3 |
H5NO (mp-625927) | 0.5596 | 0.029 | 3 |
H3CS (mp-554676) | 0.6303 | 0.047 | 3 |
H8N2O (mp-625815) | 0.4884 | 0.239 | 3 |
H6C2SBr2 (mp-860792) | 0.5749 | 0.014 | 4 |
H5BrNO (mp-23893) | 0.5991 | 0.088 | 4 |
H8C3N2O (mp-644330) | 0.5882 | 0.439 | 4 |
NaGa(H2N)4 (mp-706544) | 0.5473 | 0.006 | 4 |
LiAl(H2N)4 (mp-695962) | 0.5876 | 0.370 | 4 |
FeH16C4(NCl2)2 (mp-709074) | 0.6012 | 0.101 | 5 |
CuH12Se(NO)4 (mp-707052) | 0.6079 | 0.326 | 5 |
C2SeS2O7F6 (mp-557877) | 0.5819 | 0.233 | 5 |
AgH11C4(SO)3 (mp-560182) | 0.5182 | 0.153 | 5 |
KZnH4Br3O2 (mp-720912) | 0.5783 | 0.016 | 5 |
H8C3SN(OF)3 (mp-23777) | 0.6675 | 0.245 | 6 |
H9C3SeSN2Cl (mp-558541) | 0.6804 | 0.378 | 6 |
PH9AuC3S3Cl (mp-603254) | 0.6602 | 0.054 | 6 |
AgH8C4S3(OF)3 (mp-605808) | 0.6627 | 0.263 | 6 |
MnH12C2NCl3O2 (mp-744831) | 0.4955 | 0.486 | 6 |
CsCu3As8H24C8(IO2)4 (mp-605196) | 0.6849 | 0.136 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Al H N |
Final Energy/Atom-4.5326 eV |
Corrected Energy-259.6007 eV
Uncorrected energy = -253.8247 eV
Composition-based energy adjustment (-0.361 eV/atom x 16.0 atoms) = -5.7760 eV
Corrected energy = -259.6007 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)