material

Sr3(AlSi)2

ID:

mp-7068

DOI:

10.17188/1286261


Tags: Strontium aluminium silicide (3/2/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.401 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.16 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 100127 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 1> <0 0 1> 0.005 264.3
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.006 264.3
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.009 264.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.009 61.0
TbScO3 (mp-31119) <1 1 1> <0 0 1> 0.009 142.3
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.010 279.8
C (mp-66) <1 1 1> <0 0 1> 0.012 264.3
CdS (mp-672) <0 0 1> <0 0 1> 0.013 61.0
Bi2Se3 (mp-541837) <1 0 0> <0 1 1> 0.015 250.8
Mg (mp-153) <1 0 1> <0 0 1> 0.019 264.3
LaF3 (mp-905) <1 0 1> <1 0 0> 0.022 279.8
LaF3 (mp-905) <0 0 1> <0 0 1> 0.026 183.0
KCl (mp-23193) <1 0 0> <1 1 0> 0.027 123.6
DyScO3 (mp-31120) <1 1 1> <0 0 1> 0.027 142.3
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.030 162.7
BaTiO3 (mp-5986) <1 0 0> <0 1 1> 0.044 83.6
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.045 279.8
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.046 264.3
GaN (mp-804) <0 0 1> <0 0 1> 0.047 81.3
Al (mp-134) <1 0 0> <1 1 0> 0.050 247.2
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.052 264.3
GdScO3 (mp-5690) <1 1 1> <0 0 1> 0.054 142.3
AlN (mp-661) <1 1 1> <0 0 1> 0.056 142.3
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.059 345.7
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.059 264.3
CdSe (mp-2691) <1 1 1> <0 0 1> 0.062 264.3
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.068 223.7
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.070 264.3
Au (mp-81) <1 0 0> <0 0 1> 0.070 122.0
CdS (mp-672) <1 0 0> <0 0 1> 0.074 142.3
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.081 325.3
GaSb (mp-1156) <1 1 1> <0 0 1> 0.085 264.3
Bi2Se3 (mp-541837) <1 0 1> <0 1 1> 0.088 250.8
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.101 264.3
Ag (mp-124) <1 0 0> <0 0 1> 0.102 122.0
GaN (mp-804) <1 1 0> <0 0 1> 0.105 325.3
CdS (mp-672) <1 0 1> <0 0 1> 0.111 264.3
PbSe (mp-2201) <1 1 1> <0 0 1> 0.120 264.3
TiO2 (mp-390) <1 0 0> <1 0 0> 0.121 186.5
SiC (mp-11714) <1 1 1> <0 0 1> 0.124 162.7
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.132 142.3
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.135 345.7
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.138 142.3
GaN (mp-804) <1 0 1> <0 0 1> 0.140 264.3
MgO (mp-1265) <1 1 0> <0 0 1> 0.144 101.7
WSe2 (mp-1821) <1 1 0> <0 0 1> 0.153 264.3
GaSe (mp-1943) <0 0 1> <0 0 1> 0.157 244.0
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.167 244.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.168 244.0
CaCO3 (mp-3953) <1 0 0> <0 0 1> 0.173 264.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
71 23 18 0 0 0
23 87 21 0 0 0
18 21 111 0 0 0
0 0 0 27 0 0
0 0 0 0 34 0
0 0 0 0 0 27
Compliance Tensor Sij (10-12Pa-1)
15.6 -3.6 -1.8 0 0 0
-3.6 12.9 -1.9 0 0 0
-1.8 -1.9 9.7 0 0 0
0 0 0 36.8 0 0
0 0 0 0 29.4 0
0 0 0 0 0 36.9
Shear Modulus GV
32 GPa
Bulk Modulus KV
44 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
43 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
43 GPa
Elastic Anisotropy
0.19
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba3(AlSi)2 (mp-9578) 0.2971 0.000 3
Ca3(AlSi)2 (mp-9577) 0.2710 0.027 3
Ba3(AlSn)2 (mp-7377) 0.2297 0.006 3
Ba3(AlGe)2 (mp-10669) 0.2259 0.000 3
Sr3(AlGe)2 (mp-10671) 0.1053 0.000 3
Ti3B4 (mp-1025170) 0.6777 0.000 2
Ta5B6 (mp-28629) 0.7007 0.004 2
Mn3B4 (mp-10118) 0.7253 0.000 2
Ta3B4 (mp-10142) 0.6750 0.000 2
Nb3B4 (mp-10255) 0.7108 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Al Si
Final Energy/Atom
-3.7444 eV
Corrected Energy
-26.2111 eV
-26.2111 eV = -26.2111 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 100127
Submitted by
User remarks:
  • Strontium aluminium silicide (3/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)