Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.937 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.032 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPtS + K2SO4 + K2PtCl4 + KHSO4 |
Band Gap3.088 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmc21 [36] |
HallC 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 163.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 228.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 180.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 218.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 163.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 163.1 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 196.4 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 266.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 180.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 196.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 152.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 228.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 218.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 133.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 109.4 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 109.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 109.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 228.5 |
BN (mp-984) | <0 0 1> | <1 0 1> | 196.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 218.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 196.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 180.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 196.4 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 163.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 218.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 152.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 196.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 1 0> | 228.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 163.1 |
C (mp-66) | <1 0 0> | <0 1 0> | 76.2 |
C (mp-66) | <1 1 0> | <1 0 0> | 109.4 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 304.7 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 228.5 |
Mg (mp-153) | <1 1 1> | <0 1 1> | 180.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 76.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 76.2 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 163.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 266.7 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 0> | 109.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 228.5 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 266.7 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 152.4 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 304.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 304.7 |
Si (mp-149) | <1 0 0> | <0 1 1> | 180.0 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 163.1 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 304.7 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 304.7 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 228.5 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 163.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.09978 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.04504 | 0.00000 | 0.00000 |
0.05447 | -0.07133 | -0.12682 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.15536 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.61 | 0.00 | 0.00 |
0.00 | 2.91 | 0.00 |
0.00 | 0.00 | 2.55 |
Dielectric Tensor εij (total) |
||
---|---|---|
5.51 | 0.00 | 0.00 |
0.00 | 5.99 | 0.00 |
0.00 | 0.00 | 5.54 |
Polycrystalline dielectric constant
εpoly∞
2.69
|
Polycrystalline dielectric constant
εpoly
5.68
|
Refractive Index n1.64 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K3HPdS2(ClO3)2 (mp-697127) | 0.1612 | 0.044 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv H Pt S Cl O |
Final Energy/Atom-5.1079 eV |
Corrected Energy-164.3179 eV
-164.3179 eV = -153.2366 eV (uncorrected energy) - 11.0813 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)