material

Mn3PtN

ID:

mp-7070

DOI:

10.17188/1286284


Tags: Manganese platinum nitride (3/1/1)

Material Details

Final Magnetic Moment
9.648 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.386 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.11 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mn2N + MnPt
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-7631) <0 0 1> <1 1 1> 0.000 107.8
SiC (mp-11714) <0 0 1> <1 1 1> 0.000 107.8
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.004 53.9
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.005 44.0
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.005 62.3
GaN (mp-804) <0 0 1> <1 1 1> 0.007 27.0
PbSe (mp-2201) <1 0 0> <1 0 0> 0.009 77.8
C (mp-66) <1 1 0> <1 1 0> 0.009 198.1
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.012 31.1
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.016 280.1
CdS (mp-672) <0 0 1> <1 1 1> 0.020 107.8
GaN (mp-804) <1 1 0> <1 1 0> 0.023 88.0
GaSb (mp-1156) <1 0 0> <1 0 0> 0.027 77.8
Au (mp-81) <1 1 0> <1 1 0> 0.029 198.1
Au (mp-81) <1 0 0> <1 0 0> 0.029 140.1
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.032 233.4
CdS (mp-672) <1 1 0> <1 1 0> 0.039 198.1
PbS (mp-21276) <1 1 1> <1 1 1> 0.043 188.7
CsI (mp-614603) <1 1 1> <1 1 1> 0.046 107.8
CsI (mp-614603) <1 1 0> <1 1 0> 0.046 88.0
CsI (mp-614603) <1 0 0> <1 0 0> 0.046 62.3
CdSe (mp-2691) <1 0 0> <1 0 0> 0.048 77.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.053 242.1
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.078 132.1
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.091 80.9
Ag (mp-124) <1 1 0> <1 1 0> 0.097 198.1
Ag (mp-124) <1 0 0> <1 0 0> 0.097 140.1
GaSe (mp-1943) <0 0 1> <1 1 1> 0.101 242.6
Ni (mp-23) <1 0 0> <1 0 0> 0.102 62.3
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.104 280.1
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.108 44.0
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.115 107.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.133 186.8
InP (mp-20351) <1 1 0> <1 1 0> 0.134 198.1
InP (mp-20351) <1 0 0> <1 0 0> 0.135 140.1
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.135 132.1
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.141 155.6
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.143 171.2
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.144 171.2
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.145 220.1
SiC (mp-8062) <1 0 0> <1 0 0> 0.150 77.8
KCl (mp-23193) <1 1 0> <1 1 0> 0.159 176.1
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.162 53.9
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.163 77.8
Mg (mp-153) <1 1 0> <1 1 0> 0.165 88.0
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.167 311.3
LiAlO2 (mp-3427) <1 1 0> <1 1 1> 0.170 323.5
Te2Mo (mp-602) <1 0 1> <1 0 0> 0.174 280.1
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.176 295.7
TiO2 (mp-390) <1 1 0> <1 1 0> 0.196 264.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
275 121 121 0 0 0
121 275 121 0 0 0
121 121 275 0 0 0
0 0 0 77 0 0
0 0 0 0 77 0
0 0 0 0 0 77
Compliance Tensor Sij (10-12Pa-1)
5 -1.5 -1.5 0 0 0
-1.5 5 -1.5 0 0 0
-1.5 -1.5 5 0 0 0
0 0 0 13 0 0
0 0 0 0 13 0
0 0 0 0 0 13
Shear Modulus GV
77 GPa
Bulk Modulus KV
173 GPa
Shear Modulus GR
77 GPa
Bulk Modulus KR
173 GPa
Shear Modulus GVRH
77 GPa
Bulk Modulus KVRH
173 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.31

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
10
U Values
--
Pseudopotentials
VASP PAW: N Mn_pv Pt
Final Energy/Atom
-8.6830 eV
Corrected Energy
-43.4152 eV
-43.4152 eV = -43.4152 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 76058

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)