Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.193 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.164 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNdH12(NO5)3 + Nd(HO)3 + CO2 + H2O + N2 |
Band Gap3.309 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 300.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 225.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 225.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 225.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 225.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 225.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 150.2 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 175.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 75.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 225.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 225.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 225.3 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 175.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 300.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 175.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 175.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 225.3 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 175.5 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 225.3 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 225.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 225.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 300.4 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 300.4 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 225.3 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 225.3 |
ZnO (mp-2133) | <1 0 0> | <1 0 -1> | 139.3 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 300.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 1> | 175.5 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 75.1 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 300.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2H2C2O5 (mp-974667) | 0.5877 | 0.044 | 4 |
Pb2Se(NO4)2 (mp-615850) | 0.6972 | 0.011 | 4 |
BaH4(CO2)3 (mp-698325) | 0.5188 | 0.129 | 4 |
NdH12(NO5)3 (mp-695894) | 0.7290 | 0.011 | 4 |
SmH8(NO5)3 (mp-740754) | 0.4438 | 0.156 | 4 |
KSmH4(N2O7)2 (mp-759030) | 0.5637 | 0.000 | 5 |
BaH8C6(N3O4)2 (mp-695996) | 0.7068 | 0.009 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 H C N O |
Final Energy/Atom-6.1346 eV |
Corrected Energy-895.3619 eV
-895.3619 eV = -858.8428 eV (uncorrected energy) - 36.5191 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)