Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.538 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.524 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 268.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 268.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 173.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 268.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 268.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 268.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 268.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 195.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 173.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 268.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 268.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 268.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 268.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 268.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 179.2 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 173.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 89.6 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 268.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 268.8 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 268.8 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 268.8 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 268.8 |
C (mp-48) | <0 0 1> | <0 1 1> | 195.3 |
C (mp-48) | <1 1 0> | <0 0 1> | 268.8 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 268.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 268.8 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 268.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 89.6 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 268.8 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 268.8 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 268.8 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 268.8 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 268.8 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 268.8 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 89.6 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 268.8 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 89.6 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 268.8 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 268.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KAl2Br7 (mp-30978) | 0.7454 | 0.000 | 3 |
RbP(HO2)2 (mp-722348) | 0.5831 | 0.074 | 4 |
KHSO4 (mp-23800) | 0.2620 | 0.000 | 4 |
BaAsHO4 (mp-23810) | 0.2509 | 0.000 | 4 |
BaPHO4 (mp-698163) | 0.5089 | 0.001 | 4 |
SrPHO4 (mp-735022) | 0.2026 | 0.001 | 4 |
RbPHO3F (mp-774810) | 0.6030 | 0.000 | 5 |
K4PH5S3O16 (mp-677192) | 0.6000 | 0.000 | 5 |
K2CaH2S2O9 (mp-23723) | 0.5846 | 0.003 | 5 |
K2Cr2AsHO10 (mp-744205) | 0.5420 | 0.000 | 5 |
K2Cr2AsHO10 (mp-744181) | 0.5406 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv H Se O |
Final Energy/Atom-5.0846 eV |
Corrected Energy-614.4247 eV
-614.4247 eV = -569.4781 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)