Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.810 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.402 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMgBHO3 + MgH2SO5 + Mg3B(OF)3 + B(HO)3 + H2O |
Band Gap0.678 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <1 0 0> | 134.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 262.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 87.6 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 142.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 262.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 262.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 262.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 160.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 175.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 134.6 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 174.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 87.6 |
BN (mp-984) | <1 0 1> | <1 0 1> | 160.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 142.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 262.7 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 174.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 262.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 262.7 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 142.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 262.7 |
InSb (mp-20012) | <1 0 0> | <1 1 0> | 174.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 142.0 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 223.5 |
SiC (mp-11714) | <1 1 0> | <1 0 1> | 160.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 262.7 |
Au (mp-81) | <1 0 0> | <1 1 0> | 174.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 262.7 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 262.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 262.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 87.6 |
ZrO2 (mp-2858) | <0 1 1> | <1 1 1> | 195.6 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 174.9 |
MgF2 (mp-1249) | <0 0 1> | <1 1 0> | 174.9 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 223.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 87.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 134.6 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 262.7 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 262.7 |
Al2O3 (mp-1143) | <1 1 0> | <0 1 0> | 111.8 |
InP (mp-20351) | <1 0 0> | <0 1 1> | 142.0 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 223.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 262.7 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 87.6 |
TiO2 (mp-390) | <1 0 1> | <1 0 1> | 160.6 |
MgF2 (mp-1249) | <1 0 0> | <1 1 0> | 174.9 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 262.7 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 262.7 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 262.7 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 262.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3(H3O5)2 (mp-627291) | 0.7116 | 0.071 | 3 |
Si2H2O3 (mp-627123) | 0.6569 | 0.611 | 3 |
Na2B4H8O11 (mp-706655) | 0.6954 | 0.001 | 4 |
Be2As(HO)9 (mp-720433) | 0.7237 | 0.000 | 4 |
CuH12N2(OF2)2 (mp-850027) | 0.7177 | 0.083 | 5 |
AsH8CN3O4 (mp-23666) | 0.6802 | 0.043 | 5 |
CsNaB4H12O13 (mp-542533) | 0.7016 | 0.009 | 5 |
SrV2P2(H4O7)2 (mp-744533) | 0.7104 | 0.104 | 5 |
ZnH8C4(N4Cl)2 (mp-600171) | 0.7091 | 0.051 | 5 |
MnP3H10C3NO9 (mp-743546) | 0.7155 | 0.113 | 6 |
Cu2H26C6S7N12O5 (mp-774726) | 0.7215 | 0.036 | 6 |
V2As3H17C4N8O17 (mp-746324) | 0.6465 | 0.089 | 6 |
Re2H6PbC(NO5)2 (mp-774283) | 0.5818 | 0.076 | 6 |
ZnH12C6S2(N5O)2 (mp-734836) | 0.7375 | 0.103 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv B H S O F |
Final Energy/Atom-5.5138 eV |
Corrected Energy-678.7716 eV
-678.7716 eV = -639.5987 eV (uncorrected energy) - 39.1729 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)