Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.752 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
BN (mp-984) | <0 0 1> | <0 1 0> | 0.021 | 152.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 0.029 | 152.3 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 0.038 | 152.3 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 0.038 | 152.3 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 0.042 | 178.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 0.042 | 307.8 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 0.059 | 274.7 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 0.069 | 137.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 0.075 | 225.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 0.076 | 307.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 0.083 | 307.8 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 0.088 | 335.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 0.092 | 307.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 0.097 | 335.1 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 0.102 | 89.2 |
C (mp-48) | <1 0 1> | <1 0 1> | 0.107 | 216.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 0.108 | 178.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 0.110 | 304.6 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 1> | 0.113 | 225.2 |
MgF2 (mp-1249) | <1 1 1> | <0 1 1> | 0.120 | 274.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 0.121 | 307.8 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 0.123 | 89.2 |
Si (mp-149) | <1 1 1> | <0 0 1> | 0.127 | 307.8 |
C (mp-66) | <1 0 0> | <0 1 0> | 0.138 | 243.7 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 0.139 | 60.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 0.143 | 89.2 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 0.144 | 225.2 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 0> | 0.163 | 243.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 0.167 | 335.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 0.175 | 152.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 0.177 | 60.9 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 0.178 | 243.7 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 0.185 | 68.7 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 0.186 | 152.3 |
BN (mp-984) | <1 1 1> | <0 1 0> | 0.194 | 274.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 0.209 | 216.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 0.213 | 216.8 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 0.226 | 213.2 |
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 0.248 | 188.6 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 0.261 | 365.5 |
YAlO3 (mp-3792) | <0 1 1> | <0 1 0> | 0.265 | 243.7 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 1> | 0.269 | 216.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 0.273 | 246.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 0.273 | 304.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 0.282 | 274.7 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 0.283 | 335.1 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 0.287 | 182.8 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 1> | 0.291 | 216.8 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 0.299 | 121.8 |
Au (mp-81) | <1 1 0> | <0 1 0> | 0.304 | 274.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
135 | 41 | 52 | 0 | 0 | 0 |
41 | 95 | 39 | 0 | 0 | 0 |
52 | 39 | 116 | 0 | 0 | 0 |
0 | 0 | 0 | 42 | 0 | 0 |
0 | 0 | 0 | 0 | 67 | 0 |
0 | 0 | 0 | 0 | 0 | 48 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.6 | -2.7 | -3.4 | 0 | 0 | 0 |
-2.7 | 13.1 | -3.2 | 0 | 0 | 0 |
-3.4 | -3.2 | 11.2 | 0 | 0 | 0 |
0 | 0 | 0 | 23.9 | 0 | 0 |
0 | 0 | 0 | 0 | 14.9 | 0 |
0 | 0 | 0 | 0 | 0 | 20.8 |
Shear Modulus GV46 GPa |
Bulk Modulus KV68 GPa |
Shear Modulus GR43 GPa |
Bulk Modulus KR65 GPa |
Shear Modulus GVRH44 GPa |
Bulk Modulus KVRH66 GPa |
Elastic Anisotropy0.38 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LuB2Ru (mp-29239) | 0.6723 | 0.000 | 3 |
LiBeB (mp-1018783) | 0.7000 | 0.000 | 3 |
BaLaSi2 (mp-1078225) | 0.5212 | 0.000 | 3 |
Y3Pt (mp-7343) | 0.6737 | 0.000 | 2 |
Fe3B (mp-973682) | 0.7009 | 0.204 | 2 |
MgSi (mp-1073795) | 0.6530 | 0.112 | 2 |
LaGe (mp-1084830) | 0.3853 | 0.000 | 2 |
NpSi (mp-19937) | 0.3578 | 0.034 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Si |
Final Energy/Atom-5.9315 eV |
Corrected Energy-47.4518 eV
-47.4518 eV = -47.4518 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)