material

Ta2C

ID:

mp-7088

DOI:

10.17188/1286550


Tags: Tantalum carbide (2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.598 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.77 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 409555 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdTe (mp-406) <1 1 1> <0 0 1> 0.000 76.1
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.000 25.4
InSb (mp-20012) <1 1 1> <0 0 1> 0.002 76.1
AlN (mp-661) <0 0 1> <0 0 1> 0.007 8.5
Au (mp-81) <1 1 1> <0 0 1> 0.007 211.4
Ni (mp-23) <1 1 1> <1 0 0> 0.008 170.9
DyScO3 (mp-31120) <1 1 1> <1 1 1> 0.017 141.0
LiNbO3 (mp-3731) <1 0 1> <1 1 1> 0.024 310.2
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.025 160.7
GaTe (mp-542812) <1 0 0> <0 0 1> 0.032 135.3
KCl (mp-23193) <1 1 1> <0 0 1> 0.036 211.4
LiAlO2 (mp-3427) <1 0 0> <1 1 1> 0.045 197.4
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.046 84.6
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.047 76.1
YAlO3 (mp-3792) <1 0 0> <1 1 0> 0.047 80.7
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.054 126.9
LaAlO3 (mp-2920) <1 0 0> <1 1 0> 0.057 215.2
TbScO3 (mp-31119) <1 1 1> <1 1 1> 0.067 141.0
GaSb (mp-1156) <1 0 0> <0 0 1> 0.072 270.6
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.073 53.1
Ag (mp-124) <1 1 1> <0 0 1> 0.075 211.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.075 270.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.084 270.6
NaCl (mp-22862) <1 0 0> <1 0 1> 0.090 194.6
LaF3 (mp-905) <0 0 1> <0 0 1> 0.091 135.3
KTaO3 (mp-3614) <1 0 0> <1 0 1> 0.094 194.6
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.105 262.2
NdGaO3 (mp-3196) <0 0 1> <1 0 1> 0.110 123.8
AlN (mp-661) <1 0 1> <1 0 1> 0.123 17.7
C (mp-48) <1 0 0> <1 0 0> 0.128 77.7
InAs (mp-20305) <1 1 1> <0 0 1> 0.129 262.2
LaF3 (mp-905) <1 0 1> <1 1 1> 0.135 141.0
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.135 155.3
NdGaO3 (mp-3196) <1 0 0> <1 0 1> 0.136 88.4
Al (mp-134) <1 0 0> <1 0 1> 0.139 194.6
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.146 155.3
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.147 177.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.150 135.3
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.159 262.2
AlN (mp-661) <1 1 1> <1 1 1> 0.169 28.2
C (mp-48) <1 0 1> <1 1 0> 0.170 80.7
SiC (mp-7631) <1 0 1> <0 0 1> 0.177 143.8
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.178 62.1
CdS (mp-672) <1 0 0> <1 0 0> 0.182 170.9
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.195 139.8
DyScO3 (mp-31120) <0 1 0> <1 1 0> 0.199 215.2
AlN (mp-661) <1 1 0> <1 1 0> 0.203 26.9
AlN (mp-661) <1 0 0> <1 0 0> 0.203 15.5
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.204 169.2
Au (mp-81) <1 1 0> <1 0 1> 0.218 123.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
464 159 141 -45 0 0
159 464 141 45 0 0
141 141 493 0 0 0
-45 45 0 125 0 0
0 0 0 0 125 -45
0 0 0 0 -45 153
Compliance Tensor Sij (10-12Pa-1)
2.8 -0.9 -0.5 1.3 0 0
-0.9 2.8 -0.5 -1.3 0 0
-0.5 -0.5 2.3 0 0 0
1.3 -1.3 0 8.9 0 0
0 0 0 0 8.9 2.6
0 0 0 0 2.6 7.3
Shear Modulus GV
146 GPa
Bulk Modulus KV
256 GPa
Shear Modulus GR
131 GPa
Bulk Modulus KR
256 GPa
Shear Modulus GVRH
138 GPa
Bulk Modulus KVRH
256 GPa
Elastic Anisotropy
0.59
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2UBr6 (mp-675438) 0.3298 0.001 3
CaPbI4 (mp-754540) 0.2324 0.001 3
BiTeCl (mp-28944) 0.2398 0.000 3
BiTeBr (mp-33723) 0.1520 0.000 3
Bi2Te2Se (mp-29666) 0.3183 0.000 3
SrLa6OsI12 (mp-567419) 0.6716 0.000 4
NaLa6OsI12 (mp-569905) 0.5821 0.000 4
LiTi(SeO)2 (mp-1072633) 0.7088 1.319 4
LiCaNiF6 (mp-608204) 0.7463 0.000 4
PbI2 (mp-574189) 0.0739 0.003 2
V2C (mp-1008632) 0.0591 0.018 2
Ta2N (mp-10196) 0.0691 0.113 2
Nb2C (mp-2318) 0.0317 0.018 2
PbI2 (mp-22893) 0.0732 0.001 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ta_pv C
Final Energy/Atom
-11.5784 eV
Corrected Energy
-34.7353 eV
Uncorrected energy = -34.7353 eV Corrected energy = -34.7353 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 618840
  • 409555
Submitted by
User remarks:
  • Tantalum carbide (2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)