Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.637 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 259.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 259.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 303.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 159.5 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 199.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 292.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 179.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 179.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 318.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 219.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 59.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 292.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 99.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 179.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 318.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 279.1 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 119.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 179.4 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 219.3 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 233.3 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 219.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 219.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 159.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 219.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 338.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 311.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 338.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 292.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 279.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 179.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 159.5 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 199.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 292.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 338.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 99.7 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 106.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 233.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 279.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 338.9 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 217.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 318.9 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 227.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 151.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 219.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 318.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 139.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 159.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 99.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 358.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 99.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TmSnGe (mp-1025129) | 0.4234 | 0.000 | 3 |
ErSnGe (mp-1071492) | 0.4619 | 0.000 | 3 |
HoSnGe (mp-1077485) | 0.3717 | 0.000 | 3 |
TbSnGe (mp-1077556) | 0.4353 | 0.000 | 3 |
DySnGe (mp-1080405) | 0.4977 | 0.000 | 3 |
YbBi2 (mp-1024947) | 0.4068 | 0.000 | 2 |
UGe2 (mp-1071400) | 0.3801 | 0.110 | 2 |
UGe2 (mp-16373) | 0.3001 | 0.110 | 2 |
CaBi2 (mp-1077466) | 0.3395 | 0.000 | 2 |
EuBi2 (mp-1077479) | 0.3150 | 0.000 | 2 |
Hg (mp-1077098) | 0.7318 | 0.020 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 Sb |
Final Energy/Atom-3.9030 eV |
Corrected Energy-23.4183 eV
-23.4183 eV = -23.4183 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)