material

CoO

ID:

mp-19079

DOI:

10.17188/1193863


Tags: Cobalt(II) oxide Cobalt oxide Cobalt oxide - Li-doped

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.373 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.037 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.31 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoO
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 9865 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al2O3 (mp-1143) <1 1 0> <1 0 0> -1.527 109.8
Te2W (mp-22693) <0 1 1> <1 0 0> -1.410 292.9
BN (mp-984) <1 0 1> <1 0 0> -1.341 219.7
InAs (mp-20305) <1 1 1> <1 0 0> -0.941 329.5
CdS (mp-672) <0 0 1> <1 0 0> -0.940 91.5
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> -0.938 91.5
ZnTe (mp-2176) <1 1 1> <1 0 0> -0.937 329.5
CaCO3 (mp-3953) <0 0 1> <1 0 0> -0.933 109.8
Mg (mp-153) <0 0 1> <1 0 0> -0.929 183.1
BN (mp-984) <0 0 1> <1 0 0> -0.929 54.9
InP (mp-20351) <1 1 1> <1 0 0> -0.928 183.1
C (mp-66) <1 1 1> <1 0 0> -0.926 109.8
SiO2 (mp-6930) <0 0 1> <1 0 0> -0.915 109.8
TiO2 (mp-2657) <1 1 0> <1 1 0> -0.911 77.7
PbS (mp-21276) <1 1 1> <1 0 0> -0.706 183.1
ZrO2 (mp-2858) <1 0 1> <1 0 0> -0.623 347.9
CdS (mp-672) <1 0 1> <1 1 0> -0.565 129.5
ZnO (mp-2133) <1 0 0> <1 0 0> -0.540 274.6
TeO2 (mp-2125) <0 1 0> <1 1 0> -0.525 207.1
TiO2 (mp-2657) <1 1 1> <1 1 0> -0.411 233.0
Al2O3 (mp-1143) <1 0 0> <1 1 0> -0.398 310.7
TePb (mp-19717) <1 1 0> <1 0 0> -0.389 183.1
TeO2 (mp-2125) <0 0 1> <1 0 0> -0.368 292.9
CdWO4 (mp-19387) <1 1 0> <1 0 0> -0.351 292.9
BaTiO3 (mp-5986) <1 0 1> <1 1 0> -0.349 207.1
NdGaO3 (mp-3196) <0 0 1> <1 0 0> -0.332 311.2
Ga2O3 (mp-886) <1 0 0> <1 1 1> -0.308 126.8
C (mp-48) <1 0 1> <1 0 0> -0.258 219.7
BN (mp-984) <1 1 1> <1 0 0> -0.219 201.4
Ga2O3 (mp-886) <1 1 0> <1 1 1> -0.184 222.0
GaN (mp-804) <0 0 1> <1 1 0> -0.179 181.2
Fe2O3 (mp-24972) <1 0 0> <1 1 0> -0.163 284.8
SiO2 (mp-6930) <1 1 0> <1 1 0> -0.108 284.8
SrTiO3 (mp-4651) <1 0 0> <1 0 0> -0.093 347.9
Cu (mp-30) <1 0 0> <1 1 1> -0.062 158.6
C (mp-48) <1 1 0> <1 0 0> -0.061 164.8
MgF2 (mp-1249) <1 0 1> <1 0 0> -0.047 292.9
YVO4 (mp-19133) <0 0 1> <1 1 1> -0.042 158.6
C (mp-48) <1 1 1> <1 0 0> -0.027 201.4
NdGaO3 (mp-3196) <1 0 0> <1 0 0> -0.024 347.9
CdS (mp-672) <1 0 0> <1 0 0> -0.018 146.5
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> -0.017 128.2
SiC (mp-11714) <1 1 1> <1 1 1> -0.010 222.0
Ga2O3 (mp-886) <1 1 -1> <1 0 0> -0.008 164.8
ZrO2 (mp-2858) <1 1 -1> <1 1 0> -0.007 181.2
ZnO (mp-2133) <1 1 1> <1 0 0> -0.001 292.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.000 164.8
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.001 146.5
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.002 207.1
Al (mp-134) <1 0 0> <1 0 0> 0.003 146.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
-42 375 375 0 0 0
375 -42 375 0 0 0
375 375 -42 0 0 0
0 0 0 60 0 0
0 0 0 0 60 0
0 0 0 0 0 60
Compliance Tensor Sij (10-12Pa-1)
-1.1 1.3 1.3 0 0 0
1.3 -1.1 1.3 0 0 0
1.3 1.3 -1.1 0 0 0
0 0 0 16.7 0 0
0 0 0 0 16.7 0
0 0 0 0 0 16.7
Shear Modulus GV
-47 GPa
Bulk Modulus KV
236 GPa
Shear Modulus GR
124 GPa
Bulk Modulus KR
236 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
236 GPa
Elastic Anisotropy
-6.92
Poisson's Ratio
0.42

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
U2AsSe (mp-685138) 0.0401 0.087 3
LiCo7O8 (mp-690565) 0.0474 0.104 3
Y4SiS3 (mp-677445) 0.0453 0.000 3
AgBiSe2 (mp-33618) 0.0456 0.054 3
LiBiS2 (mp-33526) 0.0477 0.012 3
LiNi6O6F (mp-765554) 0.1395 0.057 4
LiNi5O5F (mp-765891) 0.0881 0.155 4
LiNi3O3F (mp-765309) 0.0939 0.070 4
Mg30NiCO32 (mp-1098940) 0.1410 0.215 4
Mg30FeCO32 (mp-1037344) 0.1411 0.181 4
HgO (mp-545619) 0.0387 0.149 2
AlAs (mp-988940) 0.0228 0.276 2
KC (mp-1057017) 0.0404 2.334 2
CdS (mp-370) 0.0453 0.134 2
AgTe3 (mp-28246) 0.0420 0.024 2
Se (mp-7755) 0.1751 0.181 1
K (mp-998881) 0.1832 0.120 1
Te (mp-10654) 0.0518 0.047 1
S (mp-10869) 0.1907 0.626 1
P (mp-53) 0.1909 0.144 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The N-doped CoO (N-CoO) films were prepared by electrolysis of an N2-saturated 0.05M solution of CoCl2 in acetonitrile at 1.0V (vs. Ag/AgCl), which produced a black film on the cathodic ITO surface [...]
CoOMoO3/MgO and NiOMoO3/MgO catalysts were prepared from MoO3/MgO by impregnation with methanol solutions of Co nitrate and Ni nitrate, respectively, followed by calcination at 350C. The texture of [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition CoO.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Co O
Final Energy/Atom
-6.1131 eV
Corrected Energy
-29.1024 eV
Uncorrected energy = -24.4524 eV Composition-based energy adjustment (-0.687 eV/atom x 2.0 atoms) = -1.3740 eV Composition-based energy adjustment (-1.638 eV/atom x 2.0 atoms) = -3.2760 eV Corrected energy = -29.1024 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53058
  • 245320
  • 29226
  • 53929
  • 245324
  • 29049
  • 61326
  • 245321
  • 245319
  • 174027
  • 245323
  • 76638
  • 17013
  • 53059
  • 28505
  • 191775
  • 28506
  • 53057
  • 245322
  • 624580
  • 9865
  • 624575
  • 191776
  • 29081
Submitted by
User remarks:
  • Cobalt oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)