Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.959 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoO3 |
Band Gap0.505 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 138.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 304.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 193.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 239.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 83.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 166.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 187.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 140.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 276.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 221.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 239.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 286.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 83.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 249.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 307.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 309.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 246.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 307.9 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 143.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 83.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 143.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 332.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 83.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 184.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 249.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 239.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 239.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 93.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 234.8 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 328.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 276.9 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 201.0 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 307.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 359.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 276.9 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 234.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 272.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 192.4 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 307.9 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 309.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 334.7 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 268.1 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 184.8 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 234.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 304.6 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 193.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 334.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 239.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 249.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 286.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VO2F (mp-764315) | 0.5998 | 0.079 | 3 |
VOF3 (mp-764241) | 0.6911 | 0.029 | 3 |
Tc(CO)5 (mp-680571) | 0.7220 | 0.211 | 3 |
MoNCl3 (mp-23396) | 0.7151 | 0.000 | 3 |
NbO2F (mp-766094) | 0.5969 | 0.067 | 3 |
BrN(OF2)2 (mp-555071) | 0.7479 | 0.061 | 4 |
CsUV3O11 (mp-699604) | 0.7312 | 0.008 | 4 |
MoO3 (mp-715574) | 0.6059 | 0.059 | 2 |
Explore more synthesis descriptions for materials of composition MoO3.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Mo_pv O |
Final Energy/Atom-6.9716 eV |
Corrected Energy-134.0976 eV
-134.0976 eV = -111.5461 eV (uncorrected energy) - 14.1240 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)