material

MoO2

ID:

mp-715482

DOI:

10.17188/1287051


Material Details

Final Magnetic Moment
2.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.766 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.256 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
MoO2
Band Gap
0.962 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P1 [2]
Hall
-P 1
Point Group
1
Crystal System
triclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZrO2 (mp-2858) <0 0 1> <1 1 -1> 0.003 330.9
Cu (mp-30) <1 0 0> <0 0 1> 0.012 275.2
CeO2 (mp-20194) <1 1 0> <0 1 -1> 0.012 169.4
Si (mp-149) <1 1 0> <0 1 -1> 0.012 169.4
GaN (mp-804) <0 0 1> <0 0 1> 0.015 240.8
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.020 172.0
KCl (mp-23193) <1 1 1> <0 1 -1> 0.029 282.3
LiAlO2 (mp-3427) <0 0 1> <1 1 -1> 0.032 330.9
LaF3 (mp-905) <0 0 1> <0 0 1> 0.037 137.6
BaF2 (mp-1029) <1 1 0> <0 1 -1> 0.047 56.5
Mg (mp-153) <1 0 0> <1 1 -1> 0.050 66.2
TbScO3 (mp-31119) <1 1 0> <0 1 0> 0.052 316.3
NaCl (mp-22862) <1 0 0> <1 1 0> 0.053 161.7
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.053 105.9
PbS (mp-21276) <1 0 0> <1 1 0> 0.054 323.4
KTaO3 (mp-3614) <1 0 0> <1 1 0> 0.059 80.9
SiO2 (mp-6930) <0 0 1> <0 1 1> 0.068 325.0
MgO (mp-1265) <1 0 0> <1 1 0> 0.075 161.7
Al (mp-134) <1 0 0> <1 1 0> 0.078 80.9
BN (mp-984) <0 0 1> <0 1 1> 0.081 81.3
Te2W (mp-22693) <1 0 1> <1 1 0> 0.089 202.1
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.091 80.9
AlN (mp-661) <1 0 1> <0 1 -1> 0.097 282.3
KCl (mp-23193) <1 0 0> <1 1 0> 0.099 40.4
Ni (mp-23) <1 0 0> <1 1 0> 0.100 161.7
AlN (mp-661) <0 0 1> <0 0 1> 0.101 34.4
Mg (mp-153) <1 1 1> <0 0 1> 0.102 240.8
NdGaO3 (mp-3196) <0 1 0> <0 1 -1> 0.105 169.4
Mg (mp-153) <1 1 0> <0 0 1> 0.106 172.0
GaP (mp-2490) <1 1 0> <0 1 -1> 0.107 169.4
Cu (mp-30) <1 1 0> <0 1 -1> 0.110 56.5
GaTe (mp-542812) <0 0 1> <0 1 -1> 0.112 225.8
BN (mp-984) <1 1 0> <1 1 0> 0.112 202.1
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.116 137.6
InP (mp-20351) <1 0 0> <1 1 0> 0.118 323.4
NdGaO3 (mp-3196) <1 0 1> <0 1 0> 0.119 105.4
GdScO3 (mp-5690) <1 1 0> <0 1 0> 0.121 316.3
WS2 (mp-224) <1 1 1> <0 0 1> 0.129 240.8
Au (mp-81) <1 1 0> <0 1 -1> 0.141 225.8
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.142 103.2
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.153 137.6
CdWO4 (mp-19387) <1 0 0> <0 1 -1> 0.154 282.3
CaF2 (mp-2741) <1 1 0> <0 1 -1> 0.159 169.4
WS2 (mp-224) <1 1 0> <0 0 1> 0.163 309.6
ZnO (mp-2133) <1 1 1> <1 1 0> 0.166 161.7
ZnO (mp-2133) <1 0 1> <0 0 1> 0.166 137.6
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.167 172.0
BN (mp-984) <1 0 0> <0 1 0> 0.167 175.7
LiTaO3 (mp-3666) <0 0 1> <0 1 -1> 0.167 282.3
KP(HO2)2 (mp-23959) <1 1 0> <0 0 1> 0.171 137.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
142 37 47 -5 -2 -10
37 153 41 -16 4 10
47 41 156 -4 5 20
-5 -16 -4 37 20 -3
-2 4 5 20 44 -6
-10 10 20 -3 -6 29
Compliance Tensor Sij (10-12Pa-1)
9.1 -1.8 -3.2 -0.5 1.9 6.4
-1.8 8 -1 4.5 -3 -2.8
-3.2 -1 8.7 0.7 -2.2 -7.3
-0.5 4.5 0.7 38.2 -17.6 -2.2
1.9 -3 -2.2 -17.6 31.8 7.9
6.4 -2.8 -7.3 -2.2 7.9 43.8
Shear Modulus GV
44 GPa
Bulk Modulus KV
78 GPa
Shear Modulus GR
32 GPa
Bulk Modulus KR
73 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
75 GPa
Elastic Anisotropy
1.90
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Fe(CoO3)2 (mp-761530) 0.2288 0.112 3
FeCoO4 (mp-771871) 0.2336 0.153 3
Fe3Co7O20 (mp-778275) 0.2387 0.101 3
Fe2Co3O10 (mp-778217) 0.1892 0.126 3
Mn3FeO8 (mp-771261) 0.2297 0.101 3
V3Cr3(WO8)2 (mp-775969) 0.4437 0.098 4
Mn3Cr3(WO8)2 (mp-778921) 0.3932 0.086 4
Mn3V2Co3O16 (mp-770130) 0.4480 0.122 4
Mn3V2Cr3O16 (mp-773144) 0.4253 0.084 4
Mn3Cr3(TeO8)2 (mp-772458) 0.4408 0.082 4
FeO2 (mvc-11993) 0.2526 0.258 2
MoO2 (mp-635966) 0.2573 0.229 2
VO2 (mp-634430) 0.2601 0.378 2
CrO2 (mp-714929) 0.2547 0.185 2
VO2 (mvc-11624) 0.2160 0.162 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

All of the chemical reagents were analytical grade and used as received without further purification. Graphite oxide (GO) was synthesized by a modified Hummers method [24]. MoO2-Fe3O4/G composite was [...]
3,4-Dihydroxy-3-cyclobutene-1,2-dione (squaric acid, H2Sq, 98%) was obtained from Hulls-Marl (Germany) and was thoroughly re-crystallized before use. Guanidinium carbonate Gua2CO3 (purum, 97%, Fluka [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition MoO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mo: 4.38 eV
Pseudopotentials
VASP PAW: Mo_pv O
Final Energy/Atom
-7.1541 eV
Corrected Energy
-104.1537 eV
Uncorrected energy = -85.8497 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Composition-based energy adjustment (-3.202 eV/atom x 4.0 atoms) = -12.8080 eV Corrected energy = -104.1537 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)