Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.573 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.140 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr5O12 + O2 |
Band Gap0.427 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 277.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 161.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 51.9 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 259.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 121.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 88.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 161.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 222.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 207.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 152.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 323.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 88.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 121.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 201.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 55.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 259.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 242.2 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 176.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 121.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 88.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 323.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 207.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 161.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 222.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 166.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 55.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 121.1 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 228.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 201.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 201.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 166.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 161.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 55.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 244.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 263.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 121.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 201.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 282.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 201.9 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 259.6 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 176.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 323.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 263.1 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 328.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 228.1 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 263.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 263.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni(SO4)2 (mp-850515) | 0.3607 | 0.172 | 3 |
Sb(SO4)2 (mp-760060) | 0.4445 | 0.008 | 3 |
Sn(SO4)2 (mp-759223) | 0.4016 | 0.000 | 3 |
Zr(MoO4)2 (mp-627151) | 0.3908 | 0.112 | 3 |
V(SO4)2 (mp-850087) | 0.4236 | 0.000 | 3 |
K2CdP2O7 (mp-554382) | 0.6281 | 0.000 | 4 |
SbP(OF3)2 (mp-554701) | 0.6333 | 0.000 | 4 |
Cs2GaP3O10 (mp-562504) | 0.5992 | 0.000 | 4 |
Na3V(SO4)3 (mp-562720) | 0.6329 | 0.013 | 4 |
VSO4F3 (mp-768093) | 0.5118 | 0.067 | 4 |
Cr3O8 (mp-782705) | 0.3966 | 0.115 | 2 |
Cr3O8 (mp-641815) | 0.0083 | 0.140 | 2 |
Cr3O8 (mp-715515) | 0.0745 | 0.140 | 2 |
FeH4S2NO8 (mp-703668) | 0.6887 | 0.000 | 5 |
LiV2S2(O4F3)2 (mp-769600) | 0.7387 | 0.050 | 5 |
K2MnSO4F3 (mp-18838) | 0.7363 | 0.025 | 5 |
K2MnSO4F3 (mp-19304) | 0.6745 | 0.133 | 5 |
Rb2MnSO4F3 (mp-19488) | 0.7057 | 0.000 | 5 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.7132 | 0.030 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv O |
Final Energy/Atom-6.7443 eV |
Corrected Energy-85.8451 eV
-85.8451 eV = -74.1878 eV (uncorrected energy) - 6.0390 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)