Final Magnetic Moment2.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.804 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 |
Band Gap0.530 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 275.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 216.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 170.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 222.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 301.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 144.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 275.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 170.4 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 150.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 170.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 303.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 164.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 235.9 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 225.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 367.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 275.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 209.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 249.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 170.4 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 173.4 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 150.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 209.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 157.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 216.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 170.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 196.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 216.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 288.3 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 275.2 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 209.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 157.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 131.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 235.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 173.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 314.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 222.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 275.2 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 130.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 164.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 235.9 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 225.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 78.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 164.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 86.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 144.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 205.8 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 303.5 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 192.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 205.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 65.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(O2F)2 (mp-780093) | 0.2681 | 0.643 | 3 |
Mn2O3F (mp-780038) | 0.2582 | 0.081 | 3 |
BaSrI4 (mp-752514) | 0.2471 | 0.027 | 3 |
Ni6OF11 (mp-776653) | 0.2231 | 0.038 | 3 |
Cu(SbO3)2 (mp-554658) | 0.2392 | 0.004 | 3 |
LiFe3(OF3)2 (mp-779990) | 0.2469 | 0.005 | 4 |
LiV3(OF3)2 (mp-868491) | 0.2722 | 0.000 | 4 |
LiCo3(OF3)2 (mp-850982) | 0.2536 | 0.022 | 4 |
LiV3(OF3)2 (mp-766156) | 0.2780 | 0.082 | 4 |
AlSb(WO4)2 (mvc-665) | 0.2827 | 0.181 | 4 |
TiO2 (mp-766454) | 0.2444 | 0.065 | 2 |
MnO2 (mp-715549) | 0.1673 | 0.004 | 2 |
CaCl2 (mp-23214) | 0.2342 | 0.000 | 2 |
ZrO2 (mp-776386) | 0.2042 | 0.088 | 2 |
CeSe2 (mp-1080307) | 0.1843 | 0.086 | 2 |
Explore more synthesis descriptions for materials of composition MnO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv O |
Final Energy/Atom-7.1279 eV |
Corrected Energy-73.4074 eV
-73.4074 eV = -64.1511 eV (uncorrected energy) - 5.0426 eV (MP Advanced Correction) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)