Final Magnetic Moment2.755 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.375 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.040 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + V2O5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 273.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 303.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 303.0 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 151.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 265.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 273.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 136.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 228.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 227.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 319.2 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 228.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 319.2 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 265.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 227.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 227.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 319.2 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 319.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 265.3 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 227.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 151.5 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 75.8 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 136.8 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 136.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 319.2 |
BN (mp-984) | <1 0 0> | <1 1 0> | 176.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 182.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 303.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 227.3 |
Al (mp-134) | <1 0 0> | <1 1 0> | 265.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 227.3 |
Al (mp-134) | <1 1 1> | <1 0 0> | 227.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 265.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 136.8 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 136.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 182.4 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 319.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 319.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 319.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 319.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 227.3 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 227.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 136.8 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 228.0 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 273.6 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 319.2 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 228.0 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 319.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 319.2 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 227.3 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 227.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ti4Bi2O11 (mp-559154) | 0.4696 | 0.005 | 3 |
TiNb2O7 (mp-758243) | 0.5046 | 0.022 | 3 |
V3CoO8 (mp-776864) | 0.5182 | 0.248 | 3 |
TiV3O8 (mp-849354) | 0.5026 | 0.029 | 3 |
TiNb2O7 (mp-759307) | 0.4636 | 0.005 | 3 |
Li2V4OF12 (mp-766147) | 0.7407 | 0.165 | 4 |
LiV4O5F7 (mp-777719) | 0.6939 | 0.156 | 4 |
Li2V4O5F8 (mp-764711) | 0.5335 | 0.073 | 4 |
LiV4O5F7 (mp-849984) | 0.7151 | 0.040 | 4 |
LiV4O5F7 (mp-782707) | 0.7281 | 0.094 | 4 |
V6O13 (mp-566482) | 0.1619 | 0.060 | 2 |
V6O13 (mp-714921) | 0.3084 | 0.064 | 2 |
V6O13 (mp-18896) | 0.3541 | 0.018 | 2 |
V6O13 (mp-870306) | 0.3224 | 0.051 | 2 |
V6O13 (mp-715560) | 0.3477 | 0.028 | 2 |
Na2LiLa3Ti6O18 (mp-676447) | 0.7093 | 0.025 | 5 |
Na11La7Th2Ti20O60 (mp-686371) | 0.7176 | 0.017 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv O |
Final Energy/Atom-7.6171 eV |
Corrected Energy-327.8919 eV
-327.8919 eV = -289.4484 eV (uncorrected energy) - 20.1840 eV (MP Advanced Correction) - 18.2595 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)