Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.398 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbH3(SeO3)2 |
Band Gap3.789 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 152.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 305.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 152.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 305.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 76.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 305.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 152.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 229.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 76.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 247.9 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 305.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 152.7 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 76.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 305.4 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 123.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 152.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 305.4 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 76.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 145.6 |
Si (mp-149) | <1 0 0> | <0 0 1> | 152.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 305.4 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 145.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 305.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 305.4 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 152.7 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 145.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 152.7 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 305.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 305.4 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 152.7 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 76.3 |
C (mp-48) | <1 0 0> | <0 1 0> | 247.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 305.4 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 152.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 152.7 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 76.3 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 247.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 123.9 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 229.0 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 305.4 |
MgF2 (mp-1249) | <1 0 0> | <0 1 1> | 145.6 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 123.9 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 305.4 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 229.0 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 305.4 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 76.3 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 152.7 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 229.0 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 229.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HgSeO3 (mp-557224) | 0.6389 | 0.000 | 3 |
P(HO)3 (mp-625207) | 0.7168 | 0.134 | 3 |
SrH4O3 (mp-626755) | 0.7404 | 0.037 | 3 |
Ba(H2O3)2 (mp-625964) | 0.7434 | 0.047 | 3 |
H6CN4O3 (mp-643099) | 0.6119 | 0.829 | 4 |
LaHSe3O10 (mp-765350) | 0.7212 | 0.000 | 4 |
RbH3(SeO3)2 (mp-24022) | 0.4512 | 0.000 | 4 |
HgHClO4 (mp-24294) | 0.6472 | 0.000 | 4 |
KHSeO3 (mp-24433) | 0.6175 | 0.015 | 4 |
Br2O3 (mp-28933) | 0.6467 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv H Se O |
Final Energy/Atom-4.9947 eV |
Corrected Energy-512.4708 eV
Uncorrected energy = -479.4948 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Corrected energy = -512.4708 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)