Final Magnetic Moment6.028 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.634 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.765 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 52.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 312.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 151.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 208.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 156.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 208.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 312.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 208.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 312.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 208.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 208.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 260.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 208.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 52.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 151.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 208.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 208.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 104.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 208.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 260.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 156.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 208.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 208.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 260.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 208.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 156.4 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 312.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 312.7 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 151.4 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 208.5 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 52.1 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 260.6 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 208.5 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 208.5 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 312.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 312.7 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 156.4 |
Si (mp-149) | <1 0 0> | <1 0 1> | 151.4 |
Si (mp-149) | <1 1 0> | <0 0 1> | 208.5 |
Si (mp-149) | <1 1 1> | <0 0 1> | 52.1 |
Au (mp-81) | <1 1 1> | <0 0 1> | 208.5 |
C (mp-48) | <1 0 0> | <0 0 1> | 208.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 208.5 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 312.7 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 260.6 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 156.4 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 312.7 |
CaF2 (mp-2741) | <1 0 0> | <1 0 1> | 151.4 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 208.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv H I N |
Final Energy/Atom-5.1923 eV |
Corrected Energy-401.1098 eV
Uncorrected energy = -394.6118 eV
Composition-based energy adjustment (-0.361 eV/atom x 18.0 atoms) = -6.4980 eV
Corrected energy = -401.1098 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)