Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.698 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.200 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 283.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 296.5 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 269.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 211.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 211.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 235.5 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 267.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 296.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 188.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 211.8 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 267.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 127.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 338.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 317.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 127.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 238.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 254.2 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 94.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 235.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 296.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 169.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 314.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 296.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 296.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 314.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 235.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 235.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 211.8 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 235.5 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 235.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 169.4 |
BN (mp-984) | <1 0 0> | <0 1 1> | 267.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 254.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 314.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 296.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 296.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 296.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 296.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 211.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 127.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 338.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 211.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 235.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 314.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 211.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 296.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 314.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 314.0 |
TeO2 (mp-2125) | <1 1 1> | <1 1 -1> | 103.4 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 133.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H4N2O3 (mp-626006) | 0.6003 | 0.711 | 3 |
H4N2O3 (mp-625994) | 0.5768 | 0.701 | 3 |
MoCl3O (mp-25062) | 0.5968 | 0.044 | 3 |
Li3H3N2 (mp-977164) | 0.6304 | 0.029 | 3 |
LiH2N (mp-1087524) | 0.6031 | 0.096 | 3 |
BaH4(IO)2 (mp-24090) | 0.5441 | 0.001 | 4 |
SrH2I2O (mp-703295) | 0.5422 | 0.000 | 4 |
RbLi(H2N)2 (mp-510073) | 0.5009 | 0.000 | 4 |
NaH4IO2 (mp-696512) | 0.5025 | 0.014 | 4 |
KH2I3O (mp-696649) | 0.5070 | 0.005 | 4 |
H2S (mp-721582) | 0.6200 | 0.012 | 2 |
SeBr (mp-570589) | 0.6621 | 0.006 | 2 |
H2S (mp-696805) | 0.6517 | 0.000 | 2 |
H2S (mp-33024) | 0.6340 | 0.011 | 2 |
SCl2 (mp-28128) | 0.5625 | 0.053 | 2 |
K2Cu5H8(Cl4O3)2 (mp-707879) | 0.7333 | 0.044 | 5 |
NaH4CNO2 (mp-632685) | 0.6342 | 0.203 | 5 |
LiCuH4Cl3O2 (mp-722280) | 0.7181 | 0.012 | 5 |
NaH4CNO2 (mp-706281) | 0.4436 | 0.160 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Ca_sv H N |
Final Energy/Atom-4.9163 eV |
Corrected Energy-216.3166 eV
-216.3166 eV = -216.3166 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)