Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.559 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.403 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH8S(NO2)2 + Au2S + S8O + HCNO + H4NCl + CO2 + N2 |
Band Gap3.328 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPcca [54] |
Hall-P 2a 2ac |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 185.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 308.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 308.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 185.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 308.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 308.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 246.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 61.7 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 145.8 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 264.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 264.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 185.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 132.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 308.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 145.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 153.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 308.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 61.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 246.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 308.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 185.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 185.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 185.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 153.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 308.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 246.6 |
C (mp-66) | <1 1 0> | <0 1 1> | 145.8 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 308.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 308.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 308.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 185.0 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 264.3 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 185.0 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 153.3 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 153.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 308.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 308.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 308.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 308.3 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 308.3 |
Au (mp-81) | <1 1 0> | <0 1 1> | 145.8 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 246.6 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 246.6 |
C (mp-48) | <1 0 0> | <0 0 1> | 308.3 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 246.6 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 185.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 308.3 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 308.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 132.1 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 308.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H4N2O3 (mp-24834) | 0.5376 | 0.161 | 3 |
H4N2O3 (mp-23790) | 0.5682 | 0.191 | 3 |
H4N2O3 (mp-707104) | 0.4763 | 0.171 | 3 |
H4N2O3 (mp-632734) | 0.5664 | 0.167 | 3 |
H13(C5N)2 (mp-605048) | 0.6834 | 0.144 | 3 |
HgC2O2F3 (mp-558982) | 0.5420 | 0.128 | 4 |
H9C3N3O2 (mp-556151) | 0.4993 | 0.077 | 4 |
H5C2NO (mp-697242) | 0.5478 | 0.057 | 4 |
LiH2CO3 (mp-644256) | 0.5603 | 0.456 | 4 |
H5CNO2 (mp-555229) | 0.5073 | 0.047 | 4 |
C2F (mp-683965) | 0.6929 | 0.242 | 2 |
HC (mp-995197) | 0.6134 | 0.109 | 2 |
C7F3 (mp-645316) | 0.6952 | 0.255 | 2 |
CF2 (mp-559432) | 0.6734 | 0.246 | 2 |
C37F21 (mp-555948) | 0.6831 | 0.233 | 2 |
BH6CN3F4 (mp-862539) | 0.4431 | 0.004 | 5 |
ReH6CN3O4 (mp-974606) | 0.3339 | 0.012 | 5 |
H8CS(NO)4 (mp-690771) | 0.5306 | 0.067 | 5 |
HC5N3(OF4)2 (mp-707177) | 0.5358 | 0.048 | 5 |
BH10C2N5O3 (mp-734069) | 0.5513 | 0.010 | 5 |
ZnPH7C2N4O5 (mp-699466) | 0.4878 | 0.017 | 6 |
Li2H12C3SN6O7 (mp-722272) | 0.4639 | 0.001 | 6 |
ZnH12C2S2(N3O4)2 (mp-696851) | 0.4003 | 0.019 | 6 |
ZnP2H14C2(NO)6 (mp-757310) | 0.4832 | 0.050 | 6 |
ZnH12C3S4(N3O2)2 (mp-774708) | 0.3815 | 0.043 | 6 |
H16AuC6S2N4ClO4 (mp-705526) | 0.4605 | 0.381 | 7 |
PH9C3S2NClO4 (mp-559704) | 0.6937 | 0.340 | 7 |
PH6C2S2N(ClO2)2 (mp-555563) | 0.6768 | 0.344 | 7 |
MnP2H36C12N6(ClO)2 (mp-743961) | 0.6513 | 0.117 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H Au C S N Cl O |
Final Energy/Atom-5.3109 eV |
Corrected Energy-483.9062 eV
-483.9062 eV = -467.3619 eV (uncorrected energy) - 16.5443 eV (MP Anion Correction)
|