Final Magnetic Moment1.028 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.797 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.250 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 196.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 326.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 326.9 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 198.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 60.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 196.1 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 297.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 326.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 258.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 292.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 223.3 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 267.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 181.3 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 223.1 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 267.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 326.9 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 292.3 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 297.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 219.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 302.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 267.1 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 148.9 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 294.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 219.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 219.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 181.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 111.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 223.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 181.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 326.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 198.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 267.1 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 294.2 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 326.9 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 292.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 292.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 -1> | 297.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 326.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 302.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 223.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 181.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 219.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 223.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 292.3 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 241.7 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 241.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 241.7 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 178.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 326.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 1> | 267.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3(H3O5)2 (mp-627291) | 0.5013 | 0.071 | 3 |
PH8N3O2 (mp-697683) | 0.6893 | 0.000 | 4 |
Al2Si2H4O9 (mp-720262) | 0.7162 | 0.726 | 4 |
CrP(HO)5 (mp-541142) | 0.4156 | 0.120 | 4 |
Li2Cr(H2O3)2 (mp-541476) | 0.7191 | 0.019 | 4 |
CuP(HO)5 (mp-505785) | 0.4774 | 0.174 | 4 |
CuPH6NO5 (mp-733866) | 0.5492 | 0.041 | 5 |
LiVPH2O5 (mp-779915) | 0.5655 | 0.173 | 5 |
VPH5NO6 (mp-743872) | 0.6165 | 0.070 | 5 |
Na2P2H4N2O5 (mp-758453) | 0.6312 | 0.035 | 5 |
LiCrPH2O5 (mp-850156) | 0.5714 | 0.237 | 5 |
MnP3H10C3NO9 (mp-743546) | 0.5739 | 0.113 | 6 |
Ga3P3H6C2NO13 (mp-721128) | 0.6229 | 0.220 | 6 |
Zn2GaP3H8(NO6)2 (mp-693503) | 0.7488 | 0.288 | 6 |
Al3P3H9C2NO13 (mp-772922) | 0.7253 | 0.036 | 6 |
VH8C2N2O6F (mp-745044) | 0.6432 | 0.088 | 6 |
V2PH10C2N2O8F (mp-744631) | 0.6687 | 0.153 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv P H O F |
Final Energy/Atom-5.5568 eV |
Corrected Energy-282.3143 eV
Uncorrected energy = -266.7263 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Composition-based energy adjustment (-0.462 eV/atom x 4.0 atoms) = -1.8480 eV
Corrected energy = -282.3143 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)