Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.748 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.146 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSCl2O + SnH8(NCl3)2 + S8O + SO2 + SnCl4 + N2 |
Band Gap1.840 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 1 0> | 250.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 250.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 313.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 313.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 313.3 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 313.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 313.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 313.3 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 313.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 313.3 |
Al (mp-134) | <1 1 0> | <0 1 0> | 313.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 313.3 |
BN (mp-984) | <1 1 1> | <0 1 0> | 313.3 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 313.3 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 313.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 250.6 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 313.3 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 250.6 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 313.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 313.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 313.3 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 313.3 |
Au (mp-81) | <1 0 0> | <0 1 0> | 313.3 |
WS2 (mp-224) | <1 0 1> | <0 1 0> | 188.0 |
C (mp-48) | <1 0 0> | <0 1 0> | 313.3 |
WSe2 (mp-1821) | <1 0 0> | <0 1 0> | 313.3 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 250.6 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 313.3 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 313.3 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 188.0 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 250.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 313.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 313.3 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 313.3 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 313.3 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 313.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AsS4N4F5 (mp-559296) | 0.4901 | 0.137 | 4 |
ZrS4(N2Cl3)2 (mp-559350) | 0.6349 | 0.134 | 4 |
SbS4N4Cl5 (mp-554153) | 0.4755 | 0.168 | 4 |
AsS4N4F5 (mp-558254) | 0.4839 | 0.137 | 4 |
SnS8(N2Cl)4 (mp-566296) | 0.4896 | 0.169 | 4 |
SbH3C2(O2F3)2 (mp-698527) | 0.5479 | 0.088 | 5 |
CdAs2S18N12(OF2)6 (mp-557010) | 0.7445 | 0.146 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d H S N Cl O |
Final Energy/Atom-4.6336 eV |
Corrected Energy-347.0442 eV
-347.0442 eV = -333.6197 eV (uncorrected energy) - 13.4245 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)