material

V3Ni

ID:

mp-7226

DOI:

10.17188/1287488


Tags: Nickel vanadium (1/3)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.156 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.90 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3n [223]
Hall
-P 4n 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 647028 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 1> <1 1 1> 0.002 264.4
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.005 264.4
Al (mp-134) <1 1 1> <1 1 1> 0.006 113.3
GaSe (mp-1943) <0 0 1> <1 1 1> 0.006 37.8
Al (mp-134) <1 1 0> <1 1 0> 0.006 92.5
Au (mp-81) <1 0 0> <1 0 0> 0.006 87.2
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.012 109.0
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.017 123.4
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.024 185.0
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.032 196.3
SiC (mp-7631) <1 1 1> <1 1 0> 0.036 246.7
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.038 113.3
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.039 92.5
Mg (mp-153) <0 0 1> <1 1 1> 0.046 113.3
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.051 264.4
CdTe (mp-406) <1 1 0> <1 1 0> 0.053 61.7
ZnO (mp-2133) <0 0 1> <1 1 1> 0.054 37.8
CdTe (mp-406) <1 0 0> <1 0 0> 0.056 43.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.056 21.8
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.057 61.7
Ag (mp-124) <1 0 0> <1 0 0> 0.057 87.2
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.060 92.5
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.063 43.6
TbScO3 (mp-31119) <0 0 1> <1 1 1> 0.068 188.8
InSb (mp-20012) <1 1 0> <1 1 0> 0.072 61.7
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.073 130.8
InSb (mp-20012) <1 0 0> <1 0 0> 0.076 43.6
ZnO (mp-2133) <1 0 1> <1 0 0> 0.077 239.9
NaCl (mp-22862) <1 1 0> <1 1 0> 0.084 92.5
DyScO3 (mp-31120) <0 0 1> <1 1 1> 0.086 188.8
SiC (mp-7631) <1 1 0> <1 1 0> 0.095 246.7
SiC (mp-8062) <1 1 0> <1 1 0> 0.099 246.7
SiC (mp-8062) <1 0 0> <1 0 0> 0.105 174.4
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.105 21.8
GaAs (mp-2534) <1 1 0> <1 1 0> 0.108 92.5
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.111 151.1
AlN (mp-661) <1 0 0> <1 0 0> 0.113 283.5
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.117 92.5
TePb (mp-19717) <1 1 0> <1 1 0> 0.118 61.7
CdSe (mp-2691) <1 1 1> <1 1 1> 0.119 264.4
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.119 113.3
WS2 (mp-224) <0 0 1> <1 1 1> 0.120 113.3
WSe2 (mp-1821) <1 1 1> <1 1 1> 0.122 264.4
TePb (mp-19717) <1 0 0> <1 0 0> 0.125 43.6
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.125 308.4
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.136 92.5
Ni (mp-23) <1 1 1> <1 1 1> 0.137 151.1
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.138 92.5
PbSe (mp-2201) <1 0 0> <1 0 0> 0.142 196.3
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.143 339.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
369 117 117 0 0 0
117 369 117 0 0 0
117 117 369 0 0 0
0 0 0 75 0 0
0 0 0 0 75 0
0 0 0 0 0 75
Compliance Tensor Sij (10-12Pa-1)
3.2 -0.8 -0.8 0 0 0
-0.8 3.2 -0.8 0 0 0
-0.8 -0.8 3.2 0 0 0
0 0 0 13.3 0 0
0 0 0 0 13.3 0
0 0 0 0 0 13.3
Shear Modulus GV
96 GPa
Bulk Modulus KV
201 GPa
Shear Modulus GR
90 GPa
Bulk Modulus KR
201 GPa
Shear Modulus GVRH
93 GPa
Bulk Modulus KVRH
201 GPa
Elastic Anisotropy
0.32
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ti3Ir (mp-544) 0.0000 0.000 2
Nb3Tl (mp-569366) 0.0000 0.208 2
Nb3Rh (mp-1545) 0.0000 0.000 2
Ta3Sn (mp-30871) 0.0000 0.000 2
Nb3Si (mp-10229) 0.0000 0.112 2
Cs (mp-949029) 0.0000 0.047 1
F2 (mp-21848) 0.0000 -0.000 1
Rb (mp-974620) 0.0000 0.036 1
Cr (mp-17) 0.0000 0.081 1
W (mp-11334) 0.0000 0.087 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Ni_pv
Final Energy/Atom
-8.4142 eV
Corrected Energy
-67.3136 eV
-67.3136 eV = -67.3136 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 647028
Submitted by
User remarks:
  • Nickel vanadium (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)