Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.837 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.174 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPtCl2 + H2O + N2 |
Band Gap2.262 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 299.1 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 279.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 260.7 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 194.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 213.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 299.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 -1> | 322.2 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 -1> | 330.1 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 257.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 279.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 260.7 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 284.1 |
AlN (mp-661) | <1 1 1> | <1 -1 -1> | 330.1 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 -1> | 330.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 304.1 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 286.0 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 284.1 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 145.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 238.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 217.2 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 299.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 217.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 333.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 214.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 213.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 -1> | 322.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 223.2 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 260.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.8 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 235.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 199.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 312.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 304.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 -1> | 322.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 286.0 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 304.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 267.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 1> | 235.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 -1> | 257.3 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 0> | 286.1 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 193.0 |
Ag (mp-124) | <1 1 0> | <1 -1 0> | 171.7 |
Ag (mp-124) | <1 1 1> | <1 -1 1> | 235.8 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 291.5 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 304.1 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 304.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 242.9 |
GaSe (mp-1943) | <1 1 0> | <1 -1 1> | 235.8 |
GaSe (mp-1943) | <1 1 1> | <1 0 0> | 238.4 |
LiF (mp-1138) | <1 1 1> | <1 -1 1> | 235.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoH14N5O9 (mp-744996) | 0.3835 | 0.185 | 4 |
MnH8(NO5)2 (mp-744148) | 0.5870 | 0.135 | 4 |
ZnH2(CO2)2 (mp-709039) | 0.6034 | 0.122 | 4 |
Cu2H3NO6 (mp-766274) | 0.6026 | 0.038 | 4 |
SnH8(CO)4 (mp-561405) | 0.5841 | 0.185 | 4 |
CoH17C(NO)8 (mp-735481) | 0.4340 | 0.170 | 5 |
CoH22C3(N3O4)2 (mp-746670) | 0.4920 | 0.029 | 5 |
NiH10C2(N2O3)2 (mp-745158) | 0.5371 | 0.180 | 5 |
H22RhC3(N3O4)2 (mp-600156) | 0.5214 | 0.023 | 5 |
H22IrC3(N3O4)2 (mp-698362) | 0.5221 | 0.029 | 5 |
H48PtW6C8(NO)24 (mp-773991) | 0.5981 | 0.068 | 6 |
SiH18C2N8(OF3)2 (mp-766429) | 0.5624 | 0.088 | 6 |
MnH18C4N8(ClO)4 (mp-735514) | 0.6393 | 0.082 | 6 |
MgH40C10Br2(N2O)10 (mp-707720) | 0.5663 | 0.000 | 6 |
CoH18C4N8(ClO)4 (mp-744629) | 0.6414 | 0.036 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H Pt N Cl O |
Final Energy/Atom-5.3052 eV |
Corrected Energy-147.3620 eV
Uncorrected energy = -143.2400 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -147.3620 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)