Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.881 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 283.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 298.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 202.2 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 202.2 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 216.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 59.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 298.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 202.2 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 202.2 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 330.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 85.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 314.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 298.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 178.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 285.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 264.5 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 121.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 242.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 216.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 323.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 283.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 161.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 257.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 178.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 216.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 283.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 257.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 298.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.7 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 323.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 298.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 257.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 171.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 283.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 228.7 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 161.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 257.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 314.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 200.1 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 285.9 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 114.4 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 161.7 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 242.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 200.1 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 285.9 |
GaSe (mp-1943) | <1 0 1> | <1 1 0> | 202.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 114.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 57.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 314.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 228.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Dy2InPd2 (mp-20870) | 0.0357 | 0.000 | 3 |
Er2InPd2 (mp-12689) | 0.0301 | 0.000 | 3 |
Tb2InPd2 (mp-21052) | 0.0590 | 0.000 | 3 |
Tm2InPd2 (mp-21205) | 0.0603 | 0.000 | 3 |
Y2InPd2 (mp-1079112) | 0.0584 | 0.000 | 3 |
Zr3Ga2 (mp-30684) | 0.3191 | 0.000 | 2 |
Ta3Ga2 (mp-16756) | 0.3432 | 0.000 | 2 |
Dy3Pd2 (mp-12543) | 0.3907 | 0.000 | 2 |
Nb3Ga2 (mp-11393) | 0.3335 | 0.000 | 2 |
Gd3Pd2 (mp-22077) | 0.3416 | 0.014 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 In_d Pd |
Final Energy/Atom-5.3345 eV |
Corrected Energy-53.3452 eV
-53.3452 eV = -53.3452 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)