material

Nb6Co7

ID:

mp-7250

DOI:

10.17188/1287620


Tags: Cobalt niobium (7/6)

Material Details

Final Magnetic Moment
0.980 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.164 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 624289 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 1 1> <0 0 1> 0.002 269.0
Ag (mp-124) <1 1 1> <0 0 1> 0.011 269.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.015 269.0
PbS (mp-21276) <1 1 1> <0 0 1> 0.034 62.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.035 62.1
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.036 62.1
CdSe (mp-2691) <1 1 1> <0 0 1> 0.036 269.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.049 144.8
Au (mp-81) <1 1 1> <0 0 1> 0.075 269.0
InP (mp-20351) <1 1 1> <0 0 1> 0.105 62.1
Mg (mp-153) <0 0 1> <0 0 1> 0.108 62.1
GaN (mp-804) <0 0 1> <0 0 1> 0.113 62.1
Cu (mp-30) <1 1 1> <0 0 1> 0.120 269.0
C (mp-48) <1 1 1> <0 0 1> 0.121 269.0
AlN (mp-661) <1 1 1> <1 0 1> 0.145 258.3
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.147 227.6
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.149 144.8
CdS (mp-672) <0 0 1> <0 0 1> 0.167 62.1
C (mp-66) <1 1 1> <0 0 1> 0.171 269.0
AlN (mp-661) <1 0 1> <0 0 1> 0.173 269.0
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.185 331.0
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.189 310.4
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.197 186.2
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.199 227.6
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.202 269.0
GaN (mp-804) <1 0 0> <1 0 0> 0.219 255.0
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.232 269.0
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.259 144.8
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.263 186.2
InAs (mp-20305) <1 1 1> <0 0 1> 0.267 269.0
C (mp-66) <1 0 0> <0 0 1> 0.267 227.6
MgO (mp-1265) <1 1 0> <0 0 1> 0.273 103.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.284 310.4
Ni (mp-23) <1 1 0> <1 0 1> 0.302 258.3
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.304 269.0
InP (mp-20351) <1 1 0> <0 0 1> 0.315 248.3
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.325 331.0
Te2W (mp-22693) <0 0 1> <0 0 1> 0.349 310.4
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.373 127.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.379 82.8
BN (mp-984) <0 0 1> <0 0 1> 0.390 144.8
C (mp-48) <0 0 1> <0 0 1> 0.395 20.7
C (mp-48) <1 1 0> <0 0 1> 0.395 269.0
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.411 62.1
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.417 331.0
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.419 269.0
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.424 269.0
CdS (mp-672) <1 0 0> <0 0 1> 0.428 227.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.433 82.8
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.451 165.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
353 143 135 -3 0 0
143 353 135 3 0 0
135 135 385 0 0 0
-3 3 0 76 0 0
0 0 0 0 76 -3
0 0 0 0 -3 105
Compliance Tensor Sij (10-12Pa-1)
3.6 -1.1 -0.9 0.2 0 0
-1.1 3.6 -0.9 -0.2 0 0
-0.9 -0.9 3.2 0 0 0
0.2 -0.2 0 13.1 0 0
0 0 0 0 13.1 0.4
0 0 0 0 0.4 9.6
Shear Modulus GV
96 GPa
Bulk Modulus KV
213 GPa
Shear Modulus GR
93 GPa
Bulk Modulus KR
213 GPa
Shear Modulus GVRH
95 GPa
Bulk Modulus KVRH
213 GPa
Elastic Anisotropy
0.18
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na8In6Au11 (mp-607853) 0.7401 0.000 3
Th6Cd7 (mp-30499) 0.5527 0.013 2
Co7Mo6 (mp-567747) 0.1525 0.006 2
Cs6K7 (mp-569866) 0.3223 0.025 2
Fe7W6 (mp-1473) 0.1910 0.014 2
Fe7Mo6 (mp-569594) 0.2723 0.028 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Nb_pv Co
Final Energy/Atom
-8.6532 eV
Corrected Energy
-112.4922 eV
-112.4922 eV = -112.4922 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 624289
  • 108305
  • 102550
Submitted by
User remarks:
  • Cobalt niobium (7/6)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)