Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.364 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 1> | 127.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 194.1 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 127.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 179.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 179.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 224.8 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 179.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 127.7 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 179.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 74.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 224.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 299.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 224.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 299.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 179.1 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 74.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 299.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 299.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 224.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 299.7 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 179.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 149.9 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 179.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 74.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 224.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 103.4 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 299.7 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 74.9 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 1> | 255.4 |
Si (mp-149) | <1 0 0> | <1 1 0> | 179.1 |
C (mp-48) | <0 0 1> | <0 0 1> | 299.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 299.7 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 299.7 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 224.8 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 149.9 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 103.4 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 179.1 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 299.7 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 224.8 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 299.7 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 299.7 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 224.8 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 103.4 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 74.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 299.7 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 149.9 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 224.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg2Ni3O8 (mvc-15503) | 0.5830 | 0.063 | 3 |
Li2FeF5 (mp-776886) | 0.5546 | 0.026 | 3 |
ScBiO3 (mp-555769) | 0.5797 | 0.034 | 3 |
LaSmO3 (mp-778450) | 0.5784 | 0.067 | 3 |
Li2Fe3F8 (mp-776732) | 0.5830 | 0.618 | 3 |
Li2V2OF5 (mp-765272) | 0.5673 | 0.074 | 4 |
Li4V4(OF3)3 (mp-765901) | 0.5585 | 0.101 | 4 |
TiNb2Zn2O8 (mvc-3345) | 0.5568 | 0.120 | 4 |
Nb2Zn2WO8 (mvc-551) | 0.5680 | 0.157 | 4 |
Zn2MoWO6 (mvc-6039) | 0.5458 | 0.098 | 4 |
Ir3Se8 (mp-9888) | 0.2315 | 0.000 | 2 |
Rh9Se20 (mp-684800) | 0.5551 | 0.027 | 2 |
Te2Ir (mp-569388) | 0.6006 | 0.000 | 2 |
Rh3Se8 (mp-1407) | 0.2906 | 0.000 | 2 |
Rh3Se8 (mp-32861) | 0.3626 | 0.007 | 2 |
Li4MnSn(WO6)2 (mp-775961) | 0.5531 | 0.050 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.5653 | 0.168 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.5693 | 0.048 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.4876 | 0.036 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.4863 | 0.076 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Rh_pv |
Final Energy/Atom-4.6517 eV |
Corrected Energy-51.1686 eV
-51.1686 eV = -51.1686 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)