Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.859 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH5NO + Ca(HO)2 + RbN3 + H2O + N2 |
Band Gap4.353 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCcce [68] |
HallC 2 2 1bc |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 71.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 284.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 71.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 284.2 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 213.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 248.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 284.2 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 284.2 |
BN (mp-984) | <1 0 0> | <0 1 0> | 213.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 213.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 71.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 284.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 71.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 142.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 284.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 124.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 284.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 213.2 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 284.2 |
LaF3 (mp-905) | <1 1 0> | <0 1 0> | 284.2 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 213.2 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 284.2 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 284.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 284.2 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 213.2 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 213.2 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 284.2 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 284.2 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 71.1 |
C (mp-48) | <1 0 0> | <0 1 0> | 213.2 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 248.2 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 248.2 |
CsI (mp-614603) | <1 1 1> | <0 1 0> | 213.2 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 213.2 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 124.1 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 142.1 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 284.2 |
SrTiO3 (mp-4651) | <1 0 1> | <0 1 0> | 213.2 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 0> | 142.1 |
ZnTe (mp-2176) | <1 1 0> | <0 1 0> | 284.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Ca_sv H N O |
Final Energy/Atom-6.1294 eV |
Corrected Energy-336.4845 eV
Uncorrected energy = -330.9885 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -336.4845 eV
|