Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.327 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.369 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP43212 [96] |
HallP 4nw 2abw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 1> | 141.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 108.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 108.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 141.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 153.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 182.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 182.1 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 108.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 91.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 91.1 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 153.5 |
TeO2 (mp-2125) | <1 0 1> | <1 1 0> | 153.5 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 108.6 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 141.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 153.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.1 |
WSe2 (mp-1821) | <0 0 1> | <1 1 0> | 153.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 108.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 217.1 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 217.1 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 108.6 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 108.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CdSO4 (mp-8459) | 0.4674 | 0.000 | 3 |
Sn2(SO4)3 (mp-768939) | 0.4983 | 0.012 | 3 |
InPO4 (mp-22569) | 0.5034 | 0.003 | 3 |
FeSO4 (mp-19254) | 0.4960 | 0.000 | 3 |
VSO4 (mp-769995) | 0.4662 | 0.000 | 3 |
SrSn(PO4)2 (mp-862718) | 0.4389 | 0.000 | 4 |
Li3V(SO4)3 (mp-772425) | 0.4436 | 0.054 | 4 |
K2Cd2(SO4)3 (mp-6724) | 0.4418 | 0.000 | 4 |
Tl2Cd2(SO4)3 (mp-556819) | 0.4480 | 0.000 | 4 |
K2Ca2(SO4)3 (mp-15600) | 0.4347 | 0.000 | 4 |
Cr3O8 (mp-782705) | 0.6945 | 0.115 | 2 |
Cr5O12 (mp-19575) | 0.6866 | 0.142 | 2 |
Mn3VTe2(PO4)6 (mp-782657) | 0.5817 | 0.086 | 5 |
InPH5NO5 (mp-764968) | 0.4933 | 0.000 | 5 |
Na2LaPS2O7 (mp-640915) | 0.5696 | 0.141 | 5 |
K2In2P2HO10 (mp-733854) | 0.4418 | 0.037 | 5 |
LiVSO4F3 (mp-768092) | 0.5364 | 0.056 | 5 |
Na2Sc2P4H12C4O13 (mp-709352) | 0.6736 | 0.164 | 6 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.7448 | 0.030 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.7021 | 0.018 | 6 |
AsC4S2Cl2O2F13 (mp-560424) | 0.7228 | 0.226 | 6 |
SbTe6H12C4N(OF5)6 (mp-709549) | 0.7417 | 0.281 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv In_d P H O |
Final Energy/Atom-6.0618 eV |
Corrected Energy-464.5391 eV
-464.5391 eV = -436.4475 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)