Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.385 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.192 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH2O + H3OF + H4NF + GaF3 + N2 |
Band Gap5.217 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 218.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 234.7 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 193.6 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 225.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 322.6 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 252.9 |
TePb (mp-19717) | <1 1 0> | <0 1 -1> | 237.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 270.9 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 168.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 225.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 316.0 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 193.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 316.0 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 236.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 218.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 90.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 218.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 225.7 |
GaSe (mp-1943) | <1 1 0> | <0 1 -1> | 237.8 |
GaSe (mp-1943) | <1 1 1> | <0 1 -1> | 237.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 316.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 270.9 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 158.5 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 97.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 225.7 |
BN (mp-984) | <1 1 0> | <1 1 1> | 168.6 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 317.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 225.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 316.4 |
GaN (mp-804) | <0 0 1> | <1 -1 0> | 225.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 237.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 193.6 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 234.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 237.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 258.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 322.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 237.3 |
KCl (mp-23193) | <1 1 0> | <0 1 -1> | 237.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 225.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 252.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 315.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 322.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 322.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 270.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 194.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 316.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 225.7 |
Al (mp-134) | <1 1 0> | <1 1 1> | 252.9 |
Al (mp-134) | <1 1 1> | <0 1 0> | 258.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 316.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H8PtO6 (mp-625154) | 0.6935 | 0.081 | 3 |
Ge7H18O23 (mp-627442) | 0.6739 | 0.093 | 3 |
Ge7H18O23 (mp-627418) | 0.7365 | 0.110 | 3 |
Al(HO)3 (mp-626481) | 0.7276 | 0.069 | 3 |
H8PtO6 (mp-625208) | 0.7389 | 0.048 | 3 |
CoH12SO10 (mp-745190) | 0.5553 | 0.101 | 4 |
Ga2P3H11O13 (mp-721075) | 0.5520 | 0.023 | 4 |
FeP3(H2O3)3 (mp-746690) | 0.5780 | 0.178 | 4 |
MgP2H12O11 (mp-722397) | 0.4622 | 0.028 | 4 |
MnH4S2O9 (mp-541798) | 0.5535 | 0.166 | 4 |
NaMgP3(H4O5)2 (mp-849748) | 0.5153 | 0.000 | 5 |
TiH12N2(O2F3)2 (mp-703567) | 0.4900 | 0.107 | 5 |
MnAlP2(HO)15 (mp-763195) | 0.4536 | 0.113 | 5 |
CrH12N3(OF2)3 (mp-745188) | 0.3854 | 0.381 | 5 |
K2CoP4H10O17 (mp-764838) | 0.5278 | 0.090 | 5 |
FeH12C2S2(O2F)6 (mp-743577) | 0.6222 | 0.183 | 6 |
CaH20C4S4(NO6)2 (mp-24272) | 0.6050 | 0.177 | 6 |
CdH20C4S4(NO6)2 (mp-24273) | 0.6321 | 0.201 | 6 |
NiH44C12N8(ClO5)2 (mp-746343) | 0.5642 | 0.148 | 6 |
VH12C2S2(O2F)6 (mp-744032) | 0.6101 | 0.151 | 6 |
H24RuC7S3NCl3O4 (mp-738597) | 0.6801 | 0.206 | 7 |
NaAgH16C4S4(NO5)2 (mp-605018) | 0.6220 | 0.215 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ga_d H N O F |
Final Energy/Atom-4.8655 eV |
Corrected Energy-247.4894 eV
-247.4894 eV = -243.2757 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)