material

Li(YSi)2

ID:

mp-7350

DOI:

10.17188/1287781


Tags: Lithium yttrium silicide (1/2/2)

Material Details

Final Magnetic Moment
0.006 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.662 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.047 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.73 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiYSi + YSi
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mbm [127]
Hall
-P 4 2ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 8160 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WS2 (mp-224) <1 1 1> <1 0 1> 0.004 237.6
KCl (mp-23193) <1 0 0> <0 0 1> 0.004 205.1
C (mp-66) <1 0 0> <0 0 1> 0.005 51.3
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.005 256.4
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.016 209.9
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.027 329.8
LiGaO2 (mp-5854) <0 0 1> <1 1 1> 0.031 332.7
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.037 199.6
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.039 256.4
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.044 256.4
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.046 269.9
GaTe (mp-542812) <1 0 1> <1 1 0> 0.050 296.8
WS2 (mp-224) <1 1 0> <1 0 1> 0.050 237.6
GaTe (mp-542812) <1 0 0> <1 0 0> 0.050 90.0
NaCl (mp-22862) <1 0 0> <0 0 1> 0.054 256.4
GaN (mp-804) <1 0 0> <1 1 0> 0.057 84.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.060 209.9
WS2 (mp-224) <0 0 1> <1 0 0> 0.060 209.9
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.072 119.9
GaSe (mp-1943) <0 0 1> <1 1 1> 0.079 199.6
BN (mp-984) <1 0 1> <1 1 1> 0.081 199.6
LaF3 (mp-905) <0 0 1> <1 0 0> 0.090 90.0
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.090 256.4
BN (mp-984) <0 0 1> <1 0 0> 0.093 209.9
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.095 256.4
ZnO (mp-2133) <0 0 1> <1 0 0> 0.096 179.9
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.101 84.8
C (mp-48) <1 0 1> <1 1 1> 0.102 199.6
Mg (mp-153) <1 0 0> <1 0 0> 0.104 269.9
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.105 179.9
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.106 179.9
LaAlO3 (mp-2920) <1 0 0> <1 1 0> 0.106 212.0
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.106 205.1
AlN (mp-661) <1 0 0> <1 1 0> 0.109 127.2
PbS (mp-21276) <1 0 0> <1 0 0> 0.124 179.9
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.133 179.9
TiO2 (mp-390) <0 0 1> <0 0 1> 0.135 256.4
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.140 30.0
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.149 269.9
Al (mp-134) <1 0 0> <0 0 1> 0.151 256.4
MoS2 (mp-1434) <1 0 0> <1 0 0> 0.152 269.9
PbS (mp-21276) <1 1 0> <1 1 0> 0.153 254.4
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.158 205.1
MgO (mp-1265) <1 0 0> <1 0 0> 0.162 90.0
LiGaO2 (mp-5854) <1 1 1> <1 0 0> 0.163 329.8
GaTe (mp-542812) <0 0 1> <1 0 0> 0.164 149.9
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.167 51.3
SiC (mp-11714) <1 0 0> <1 1 0> 0.168 127.2
MgO (mp-1265) <1 1 0> <1 1 0> 0.179 127.2
Bi2Se3 (mp-541837) <1 0 0> <1 1 0> 0.179 127.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
117 55 55 0 0 0
55 100 40 0 0 0
55 40 100 0 0 0
0 0 0 59 0 0
0 0 0 0 67 0
0 0 0 0 0 67
Compliance Tensor Sij (10-12Pa-1)
13.6 -5.4 -5.4 0 0 0
-5.4 14.1 -2.7 0 0 0
-5.4 -2.7 14.1 0 0 0
0 0 0 16.9 0 0
0 0 0 0 14.9 0
0 0 0 0 0 14.9
Shear Modulus GV
50 GPa
Bulk Modulus KV
69 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
67 GPa
Shear Modulus GVRH
46 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
1.01
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ce2MgSi2 (mp-505296) 0.0836 0.000 3
La2InGe2 (mp-21288) 0.0856 0.000 3
Pr2InGe2 (mp-20715) 0.0730 0.000 3
Dy2MgSi2 (mp-570561) 0.0619 0.000 3
Nd2CdGe2 (mp-1079135) 0.0793 0.000 3
La3Si2 (mp-10162) 0.3962 0.005 2
U3Si2 (mp-21346) 0.4139 0.151 2
Np3Si2 (mp-1079895) 0.3463 0.438 2
Pu3Si2 (mp-1080146) 0.1977 0.000 2
Ce3Si2 (mp-1079007) 0.3524 0.001 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Y_sv Si
Final Energy/Atom
-5.7996 eV
Corrected Energy
-57.9963 eV
-57.9963 eV = -57.9963 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 8160
Submitted by
User remarks:
  • Lithium yttrium silicide (1/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)