Final Magnetic Moment0.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.641 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.113 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaPHO4 + VPO4 |
Band Gap1.518 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 126.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 338.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 169.2 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 211.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 296.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 338.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 211.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 211.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 338.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 211.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 211.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 211.5 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 138.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 263.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 84.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 338.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 338.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 84.6 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 131.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 211.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 253.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 211.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 211.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 296.1 |
LiNbO3 (mp-3731) | <1 1 1> | <0 1 0> | 126.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 169.2 |
Al (mp-134) | <1 0 0> | <0 1 0> | 211.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 131.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 296.1 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 138.2 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 338.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 131.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 138.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 211.5 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 211.5 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 211.5 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 169.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 211.5 |
C (mp-66) | <1 1 0> | <0 1 0> | 296.1 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 296.1 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 0> | 126.9 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 296.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 131.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 263.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 1> | 138.2 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 211.5 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 338.4 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 211.5 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 1 0> | 211.5 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 131.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg3(PO6)2 (mp-867981) | 0.5122 | 0.555 | 3 |
V3(P2O7)2 (mp-32416) | 0.6308 | 0.033 | 3 |
Fe2(TeO4)3 (mvc-7929) | 0.6389 | 0.300 | 3 |
P4W3O14 (mvc-1031) | 0.6333 | 0.315 | 3 |
Fe3(PO4)4 (mp-697810) | 0.6568 | 0.329 | 3 |
KFe3(PO6)2 (mp-863293) | 0.5109 | 0.202 | 4 |
K2Mn2(MoO4)3 (mp-651434) | 0.5685 | 0.000 | 4 |
ZnCo3(P2O7)2 (mvc-884) | 0.5922 | 0.060 | 4 |
ZnFe3(P2O7)2 (mvc-901) | 0.5759 | 0.391 | 4 |
Li3V4(PO4)6 (mp-767790) | 0.5736 | 0.062 | 4 |
Cr5O12 (mp-19575) | 0.7305 | 0.142 | 2 |
CaFe2P3HO12 (mp-744240) | 0.4119 | 0.008 | 5 |
Rb2MgP2WO10 (mp-579190) | 0.4914 | 0.000 | 5 |
K2Cr2Cd(H2O5)2 (mp-24928) | 0.5522 | 0.000 | 5 |
KScAs2(HO4)2 (mp-695800) | 0.5423 | 0.000 | 5 |
LiMn2P2HO9 (mp-780931) | 0.5033 | 0.144 | 5 |
Na2Sc2P4H12C4O13 (mp-709352) | 0.6715 | 0.164 | 6 |
KFeBP2HO9 (mp-635134) | 0.6693 | 0.112 | 6 |
InBP2H5NO9 (mp-752709) | 0.6629 | 0.000 | 6 |
RbInBP2HO9 (mp-766175) | 0.6693 | 0.000 | 6 |
RbScBP2HO9 (mp-23809) | 0.6072 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6923 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ca_sv V_pv P H O |
Final Energy/Atom-7.2324 eV |
Corrected Energy-596.8307 eV
-596.8307 eV = -549.6648 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)