Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.839 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.052 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + H2O + SrCO3 + C |
Band Gap2.910 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 258.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 296.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 197.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 137.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 221.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 221.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 295.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 295.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 296.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 137.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 99.0 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 258.5 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 296.9 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 295.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 184.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 332.3 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 295.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 296.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 99.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 295.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 221.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 332.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 221.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 99.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 137.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 221.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 221.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 332.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 184.6 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 105.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 296.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 295.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 332.3 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 295.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 221.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 258.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 137.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 137.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 258.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 184.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 221.6 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 258.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 109.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 295.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 295.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 296.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 110.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 184.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H3NO4 (mp-706430) | 0.7410 | 0.042 | 3 |
H2CO2 (mp-558412) | 0.6803 | 0.129 | 3 |
KHCO3 (mp-634431) | 0.6194 | 0.000 | 4 |
RbH3(CO2)2 (mp-23688) | 0.6213 | 0.101 | 4 |
BaH3C3O7 (mp-23755) | 0.1627 | 0.049 | 4 |
KCN3O2 (mp-558995) | 0.5355 | 0.442 | 4 |
BaH4(CO3)2 (mp-555646) | 0.5668 | 0.046 | 4 |
K2H2C2S2N2O (mp-722245) | 0.5477 | 0.091 | 6 |
AsH2C2NCl2O (mp-690847) | 0.7478 | 0.432 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv H C O |
Final Energy/Atom-6.7536 eV |
Corrected Energy-397.4385 eV
Uncorrected energy = -378.2025 eV
Composition-based energy adjustment (-0.687 eV/atom x 28.0 atoms) = -19.2360 eV
Corrected energy = -397.4385 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)