material

Rh

ID:

mp-74

DOI:

10.17188/1287920


Tags: Rhodium

Material Details

Final Magnetic Moment
0.006 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.03 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 52064 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.000 167.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.001 133.3
LiF (mp-1138) <1 1 0> <1 1 0> 0.001 188.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.001 230.4
BN (mp-984) <1 1 0> <1 1 0> 0.002 167.6
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.003 133.3
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.003 188.5
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.009 77.0
Ge (mp-32) <1 0 0> <1 0 0> 0.016 133.3
Ge (mp-32) <1 1 0> <1 1 0> 0.017 188.5
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.027 311.1
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.028 62.8
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.046 222.2
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.054 281.4
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.055 62.8
Cu (mp-30) <1 0 0> <1 0 0> 0.058 118.5
Cu (mp-30) <1 1 0> <1 1 0> 0.061 167.6
SiC (mp-7631) <1 0 1> <1 0 0> 0.066 237.0
GaAs (mp-2534) <1 0 0> <1 0 0> 0.080 133.3
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.082 83.8
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.082 222.2
GaAs (mp-2534) <1 1 0> <1 1 0> 0.085 188.5
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.094 296.2
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.098 311.1
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.106 29.6
AlN (mp-661) <0 0 1> <1 1 1> 0.107 25.7
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.111 281.4
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.112 41.9
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.115 311.1
Si (mp-149) <1 0 0> <1 0 0> 0.117 29.6
Si (mp-149) <1 1 0> <1 1 0> 0.124 41.9
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.127 281.4
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.129 251.8
InSb (mp-20012) <1 1 0> <1 1 0> 0.132 62.8
InSb (mp-20012) <1 1 1> <1 1 1> 0.134 77.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.144 133.3
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.153 188.5
CdTe (mp-406) <1 1 0> <1 1 0> 0.167 62.8
CdTe (mp-406) <1 1 1> <1 1 1> 0.171 77.0
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.184 25.7
Te2W (mp-22693) <1 0 0> <1 1 0> 0.204 293.3
C (mp-48) <1 0 1> <1 0 0> 0.208 222.2
TiO2 (mp-390) <1 0 0> <1 0 0> 0.226 74.1
LaF3 (mp-905) <0 0 1> <1 1 1> 0.231 179.6
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.237 325.9
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.248 296.2
TiO2 (mp-390) <1 1 0> <1 1 0> 0.263 104.7
C (mp-66) <1 1 1> <1 1 0> 0.316 335.2
YAlO3 (mp-3792) <1 0 1> <1 1 0> 0.324 146.6
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.325 222.2
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
2.12 J/m2 (0.13 eV/Å2)
Weighted work function Φ
4.99 eV
Shape factor η
5.16
Surface energy anisotropy αγ
0.080
Miller Indices
(hkl)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(111) 1.98, 0.12 5.15 0.60
(332) 2.16, 0.13 4.82 0.00
(322) 2.20, 0.14 4.82 0.02
(221) 2.22, 0.14 4.74 0.08
(331) 2.31, 0.14 4.57 0.00
(211) 2.31, 0.14 4.75 0.04
(110) 2.33, 0.15 4.27 0.05
(100) 2.35, 0.15 5.01 0.14
(311) 2.39, 0.15 4.65 0.07
(321) 2.41, 0.15 4.57 0.00
(320) 2.46, 0.15 4.43 0.00
(310) 2.49, 0.16 4.62 0.01
(210) 2.50, 0.16 4.52 0.00

Grain Boundaries

Reference for grain boundary energies and properties:
Sigma, Σ
type
rotation axis rotation angle GB plane Energy, 𝛾GB
(J/m2)
Work of Separation, Wsep
(J/m2)
Structure
(CIF)
3 twist [111] 60.00 (111) 0.08 3.90
3 tilt [110] 109.47 (112) 1.25 3.37
3 tilt [111] 180.00 (110) 1.55 3.11
5 twist [100] 36.87 (100) 1.17 3.48
5 tilt [100] 53.13 (013) 1.45 3.54
5 tilt [100] 36.87 (021) 1.68 3.32
7 twist [111] 38.21 (111) 0.65 3.32
7 tilt [111] 38.21 (321) 1.54 3.27
9 tilt [110] 38.94 (221) 1.31 3.14
9 twist [110] 38.94 (110) 1.85 2.81

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
397 182 182 0 0 0
182 397 182 0 0 0
182 182 397 0 0 0
0 0 0 177 0 0
0 0 0 0 177 0
0 0 0 0 0 177
Compliance Tensor Sij (10-12Pa-1)
3.5 -1.1 -1.1 0 0 0
-1.1 3.5 -1.1 0 0 0
-1.1 -1.1 3.5 0 0 0
0 0 0 5.7 0 0
0 0 0 0 5.7 0
0 0 0 0 0 5.7
Shear Modulus GV
149 GPa
Bulk Modulus KV
253 GPa
Shear Modulus GR
141 GPa
Bulk Modulus KR
253 GPa
Shear Modulus GVRH
145 GPa
Bulk Modulus KVRH
253 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.26

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -7.343 14.278 13.914 8.470
pack_evans_james -7.343 14.280 1.539 4.159
vinet -7.346 14.263 14.280 6.424
tait -7.344 14.267 1.556 6.338
birch_euler -7.344 14.272 1.756 1.211
pourier_tarantola -7.350 14.255 0.276 3.248
birch_lagrange -7.365 14.266 1.047 6.728
murnaghan -7.340 14.300 1.496 3.974
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.034 3
LiCa6Ge (mp-12609) 0.0000 0.183 3
GaFeNi2 (mp-1065359) 0.0412 0.065 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.065 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
Yb3Ti (mp-979963) 0.0000 0.402 2
ErGa3 (mp-398) 0.0000 0.000 2
NbCo3 (mp-1018021) 0.0000 0.014 2
Pr3In (mp-19764) 0.0000 0.000 2
YMg7 (mp-1079382) 0.0000 0.079 2
Na (mp-974558) 0.0000 0.003 1
Br (mp-998870) 0.0000 0.666 1
Mn (mp-8634) 0.0000 0.083 1
Pb (mp-20483) 0.0000 0.000 1
Cu (mp-30) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rh_pv
Final Energy/Atom
-7.3643 eV
Corrected Energy
-7.3643 eV
-7.3643 eV = -7.3643 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 191463
  • 64991
  • 53811
  • 650221
  • 650222
  • 76952
  • 171677
  • 52252
  • 426969
  • 650218
  • 52064
  • 41516
Submitted by
User remarks:
  • Rhodium

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)