Final Magnetic Moment1.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.689 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 289.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 144.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 208.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 270.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 255.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 144.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 -1> | 162.9 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 162.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 289.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 289.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 276.7 |
Te2Mo (mp-602) | <0 0 1> | <1 1 -1> | 251.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 293.5 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 271.5 |
Ag (mp-124) | <1 1 1> | <0 1 -1> | 325.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 195.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 270.2 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 54.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 195.6 |
AlN (mp-661) | <1 1 1> | <1 -1 0> | 232.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 293.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 271.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 -1> | 217.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 144.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 293.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 270.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 216.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 202.6 |
BN (mp-984) | <1 0 0> | <0 1 -1> | 217.2 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 170.3 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 289.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 244.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 342.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 244.5 |
BN (mp-984) | <1 1 0> | <0 1 0> | 104.0 |
BN (mp-984) | <1 1 1> | <1 0 1> | 279.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 195.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 243.1 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 251.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 216.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 271.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 251.4 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 0 1> | 244.5 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 216.9 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 -1> | 282.1 |
MoS2 (mp-1434) | <1 0 0> | <1 -1 -1> | 282.1 |
MoS2 (mp-1434) | <1 0 1> | <0 1 -1> | 271.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 184.5 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 162.9 |
Al (mp-134) | <1 1 0> | <0 1 -1> | 162.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2Cu5P4(HO9)2 (mp-745163) | 0.7318 | 0.015 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv P H O |
Final Energy/Atom-5.9731 eV |
Corrected Energy-222.7990 eV
Uncorrected energy = -209.0590 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Corrected energy = -222.7990 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)