material

Ca(CdSb)2

ID:

mp-7430

DOI:

10.17188/1287970


Tags: Calcium cadmium antimonide (1/2/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.464 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.70 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.109 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 12151 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-7631) <0 0 1> <0 0 1> 0.000 58.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.001 58.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.001 250.6
TeO2 (mp-2125) <1 1 0> <1 1 1> 0.002 196.8
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.002 287.2
YVO4 (mp-19133) <1 1 1> <1 1 0> 0.007 250.6
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.013 250.6
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.016 271.1
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.017 251.8
Ge (mp-32) <1 1 0> <1 1 0> 0.019 188.0
LaF3 (mp-905) <0 0 1> <0 0 1> 0.019 135.6
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.025 188.0
GaAs (mp-2534) <1 1 0> <1 1 0> 0.031 188.0
PbS (mp-21276) <1 1 1> <0 0 1> 0.032 251.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.038 77.5
KCl (mp-23193) <1 1 0> <1 0 1> 0.038 287.2
ZnO (mp-2133) <1 0 0> <1 0 1> 0.042 123.1
Ge (mp-32) <1 1 1> <0 0 1> 0.046 58.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.047 188.0
Al (mp-134) <1 1 1> <0 0 1> 0.048 251.8
NdGaO3 (mp-3196) <1 1 1> <1 0 1> 0.049 205.2
SiC (mp-11714) <1 0 0> <1 0 0> 0.059 253.2
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.073 125.3
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.074 328.3
Si (mp-149) <1 1 0> <1 1 0> 0.078 125.3
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.078 72.4
Te2W (mp-22693) <1 0 0> <1 0 0> 0.079 289.4
GdScO3 (mp-5690) <0 1 1> <1 1 1> 0.082 327.9
CdTe (mp-406) <1 1 0> <0 0 1> 0.093 309.9
C (mp-48) <1 0 1> <1 1 1> 0.095 262.3
GaAs (mp-2534) <1 1 1> <0 0 1> 0.096 58.1
InSb (mp-20012) <1 1 0> <0 0 1> 0.098 309.9
ZnO (mp-2133) <1 1 1> <1 0 1> 0.114 287.2
ZnO (mp-2133) <1 0 1> <1 0 0> 0.115 180.9
YVO4 (mp-19133) <0 0 1> <1 1 1> 0.119 262.3
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.120 131.2
Ni (mp-23) <1 1 1> <0 0 1> 0.121 251.8
GaN (mp-804) <1 0 1> <1 0 1> 0.122 287.2
Cu (mp-30) <1 1 0> <1 0 1> 0.122 205.2
Al (mp-134) <1 0 0> <1 1 1> 0.123 65.6
InSb (mp-20012) <1 1 1> <0 0 1> 0.124 77.5
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.136 58.1
TbScO3 (mp-31119) <0 1 1> <1 1 1> 0.137 327.9
Au (mp-81) <1 1 1> <0 0 1> 0.139 368.0
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.142 250.6
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.142 289.4
CdTe (mp-406) <1 1 1> <0 0 1> 0.144 77.5
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.150 65.6
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.151 77.5
Ag (mp-124) <1 1 0> <0 0 1> 0.152 96.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
74 28 21 -1 0 0
28 74 21 1 0 0
21 21 63 0 0 0
-1 1 0 16 0 0
0 0 0 0 16 -1
0 0 0 0 -1 23
Compliance Tensor Sij (10-12Pa-1)
16.6 -5.3 -3.8 1.1 0 0
-5.3 16.6 -3.8 -1.1 0 0
-3.8 -3.8 18.6 0 0 0
1.1 -1.1 0 62.4 0 0
0 0 0 0 62.4 2.3
0 0 0 0 2.3 43.7
Shear Modulus GV
20 GPa
Bulk Modulus KV
39 GPa
Shear Modulus GR
20 GPa
Bulk Modulus KR
39 GPa
Shear Modulus GVRH
20 GPa
Bulk Modulus KVRH
39 GPa
Elastic Anisotropy
0.20
Poisson's Ratio
0.28

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
50.78 0.00 0.00
0.00 50.78 0.00
0.00 0.00 15.86
Dielectric Tensor εij (total)
62.51 0.00 0.00
0.00 62.51 -0.00
0.00 -0.00 30.34
Polycrystalline dielectric constant εpoly
(electronic contribution)
39.14
Polycrystalline dielectric constant εpoly
(total)
51.78
Refractive Index n
6.26
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CeAs2 (mp-8152) 0.1281 0.000 3
Yb(CdSb)2 (mp-9257) 0.0305 0.000 3
Ca(MgBi)2 (mp-29208) 0.0890 0.000 3
Yb(MgBi)2 (mp-1068042) 0.0902 0.000 3
Ca(CdAs)2 (mp-7067) 0.0674 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.2546 0.040 4
LiFeCuS2 (mp-755288) 0.3009 0.262 4
Mg3As2 (mp-7891) 0.2109 0.018 2
Bi2O3 (mp-1017552) 0.3453 0.071 2
Pu2O3 (mp-21423) 0.3257 0.073 2
Mg3Bi2 (mp-569018) 0.1838 0.000 2
Mg3Sb2 (mp-2646) 0.1180 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Cd Sb
Final Energy/Atom
-2.8777 eV
Corrected Energy
-14.7723 eV
Uncorrected energy = -14.3883 eV Composition-based energy adjustment (-0.192 eV/atom x 2.0 atoms) = -0.3840 eV Corrected energy = -14.7723 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 12151
Submitted by
User remarks:
  • Calcium cadmium antimonide (1/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)