Final Magnetic Moment0.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.977 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.148 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH5CNO3 + CoCO3 + H2O + C + Co |
Band Gap2.745 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 96.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 277.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 208.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 277.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 138.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 193.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 96.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 96.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 121.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 277.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.4 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 96.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 238.2 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 119.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 208.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 277.6 |
BN (mp-984) | <1 1 1> | <0 1 1> | 238.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 138.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 121.7 |
Al (mp-134) | <1 0 0> | <0 1 0> | 96.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 138.8 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 193.6 |
CdTe (mp-406) | <1 1 1> | <0 1 1> | 238.2 |
TeO2 (mp-2125) | <1 0 1> | <1 1 1> | 155.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 139.2 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 100.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 290.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 208.2 |
TiO2 (mp-2657) | <1 0 1> | <1 1 1> | 155.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 138.8 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 290.4 |
PbS (mp-21276) | <1 1 1> | <1 0 1> | 121.7 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 96.8 |
InP (mp-20351) | <1 1 1> | <0 1 1> | 119.1 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 277.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 208.2 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 139.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 290.4 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 290.4 |
Au (mp-81) | <1 1 0> | <0 1 0> | 96.8 |
WS2 (mp-224) | <0 0 1> | <0 1 1> | 238.2 |
WS2 (mp-224) | <1 0 1> | <0 1 1> | 238.2 |
WS2 (mp-224) | <1 1 1> | <0 1 1> | 238.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 277.6 |
WSe2 (mp-1821) | <0 0 1> | <0 1 1> | 238.2 |
ZrO2 (mp-2858) | <0 0 1> | <1 1 0> | 139.2 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 138.8 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 138.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 277.6 |
SiC (mp-8062) | <1 1 1> | <0 1 1> | 238.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2Si2H4O9 (mp-721216) | 0.7418 | 0.013 | 4 |
FeH4C3O5 (mp-567010) | 0.5220 | 0.270 | 4 |
RuC4(O2F3)2 (mp-542700) | 0.5836 | 0.146 | 4 |
SnH8(CO)4 (mp-561405) | 0.6728 | 0.185 | 4 |
Al2Si2H4O9 (mp-541152) | 0.7298 | 0.013 | 4 |
MnH11C5NO6 (mp-566740) | 0.2322 | 0.207 | 5 |
MnH9C4NO6 (mp-656241) | 0.1348 | 0.235 | 5 |
MnH9C4NO6 (mp-600579) | 0.1190 | 0.337 | 5 |
Mg3H13C9NO13 (mp-605684) | 0.3946 | 0.138 | 5 |
CoH16C4(NO)7 (mp-744418) | 0.3901 | 0.348 | 5 |
NiH48C16S8(NO7)2 (mp-744812) | 0.6475 | 0.300 | 6 |
SnH58C16S4(N11O9)2 (mp-558106) | 0.6765 | 0.091 | 6 |
YH24C9N6(ClO)3 (mp-558263) | 0.4321 | 0.097 | 6 |
BH6Ru3C6O19F4 (mp-699265) | 0.6823 | 0.645 | 6 |
H14RhC6NClO4 (mp-561074) | 0.6450 | 0.150 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co H C N O |
Final Energy/Atom-5.9639 eV |
Corrected Energy-524.0044 eV
Uncorrected energy = -500.9644 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV
Corrected energy = -524.0044 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)