Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.877 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe3(PO4)4 + LiTi2(PO4)3 + Li3PO4 |
Band Gap2.432 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 327.4 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 302.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 75.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 327.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 107.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 107.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 302.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 196.4 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 251.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 151.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 196.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 196.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 107.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 250.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 261.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 302.7 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 75.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 196.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 196.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 151.4 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 214.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 196.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 261.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 250.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 227.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 131.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 196.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 214.6 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 302.7 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 75.7 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 107.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 196.4 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 302.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 196.4 |
C (mp-66) | <1 1 0> | <1 0 1> | 107.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.5 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 -1> | 304.1 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 261.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 327.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 327.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 327.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiFeF4 (mp-777472) | 0.5894 | 0.092 | 3 |
Ti5(PO5)4 (mp-559530) | 0.5094 | 0.000 | 3 |
FeMoO4 (mp-541843) | 0.5728 | 0.399 | 3 |
MgMoO4 (mp-19047) | 0.5704 | 0.000 | 3 |
MnMoO4 (mp-19081) | 0.5731 | 0.000 | 3 |
Na5V4(PO4)6 (mp-764294) | 0.3458 | 0.105 | 4 |
LiV2(PO4)3 (mp-762630) | 0.3481 | 0.054 | 4 |
LiFe2(PO4)3 (mp-997548) | 0.3424 | 0.065 | 4 |
LiV2(PO4)3 (mp-32436) | 0.3497 | 0.016 | 4 |
LiTi2(PO4)3 (mp-774539) | 0.3585 | 0.007 | 4 |
Li9Nb10Cr6(PO4)24 (mp-851292) | 0.3917 | 0.031 | 5 |
Li3Ti3Fe(PO4)6 (mp-743728) | 0.3600 | 0.013 | 5 |
ZrCrCu2(PO4)3 (mp-743605) | 0.4319 | 0.145 | 5 |
LiNbSn3(PO4)6 (mp-759486) | 0.3875 | 0.017 | 5 |
LiMgAl3(SO4)6 (mp-677680) | 0.4514 | 0.017 | 5 |
NaLi3Ti2Fe2(PO4)6 (mp-744690) | 0.5374 | 0.193 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-743387) | 0.5376 | 0.023 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5283 | 0.114 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5329 | 0.015 | 6 |
NaLi3Ti2Al2(PO4)6 (mp-776523) | 0.5039 | 0.036 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7276 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Fe_pv P O |
Final Energy/Atom-7.4583 eV |
Corrected Energy-295.5467 eV
-295.5467 eV = -275.9587 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 2.7330 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)