Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.316 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.582 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKHSO4 + MnH2SO5 + H2O |
Band Gap0.782 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 -1> | 254.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 227.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 278.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 86.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 198.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 301.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 213.0 |
KCl (mp-23193) | <1 1 0> | <1 -1 0> | 290.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 341.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 302.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 -1> | 240.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 -1> | 213.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 301.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 284.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 233.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 284.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 315.6 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 228.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 301.4 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 301.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 233.1 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 315.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 233.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 210.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 326.3 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 -1> | 169.6 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 120.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 228.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 -1 0> | 290.9 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 171.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 172.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 198.8 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 302.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 284.0 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 302.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 326.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 284.8 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 218.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 258.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 172.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 215.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 240.7 |
BN (mp-984) | <1 0 0> | <1 1 0> | 263.0 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 195.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 279.7 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 105.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 227.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 261.2 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 218.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 326.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VHO3 (mp-627119) | 0.6630 | 0.069 | 3 |
NaH5(SO4)3 (mp-734160) | 0.7374 | 0.678 | 4 |
MgH12SO9 (mp-697114) | 0.6030 | 0.309 | 4 |
CoH4SeO5 (mp-744532) | 0.6709 | 0.070 | 4 |
CaH8(BrO6)2 (mp-745067) | 0.6900 | 0.038 | 4 |
AlH18(BrO6)3 (mp-695979) | 0.7321 | 0.302 | 4 |
Br2O3 (mp-28933) | 0.7444 | 0.000 | 2 |
KFeH5(SO5)2 (mp-694884) | 0.5350 | 0.432 | 5 |
HgH2C6(NCl2)2 (mp-736545) | 0.6917 | 0.989 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: K_sv Mn_pv H S O |
Final Energy/Atom-5.2206 eV |
Corrected Energy-109.2215 eV
-109.2215 eV = -99.1908 eV (uncorrected energy) - 8.3498 eV (MP Anion Correction) - 1.6809 eV (MP Advanced Correction)
|