Final Magnetic Moment0.925 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.224 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.153 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaMn2O4 + CaTiO3 + Ho2TiO5 |
Band Gap0.540 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 151.0 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 175.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 120.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 82.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 332.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 82.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 257.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 90.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 164.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 90.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 120.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 241.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 30.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 82.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 271.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 151.0 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 171.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 87.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 211.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 90.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 211.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 262.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 164.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 257.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 90.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 257.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 90.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 271.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 271.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 257.5 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 262.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 90.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 332.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 301.9 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 164.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 175.2 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 262.7 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 182.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 164.3 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 164.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 164.3 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 273.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 332.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 301.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 332.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 332.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 271.7 |
BN (mp-984) | <1 1 0> | <1 1 0> | 238.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3Mo2O7 (mvc-3696) | 0.3307 | 0.134 | 3 |
Ca4Ta2O9 (mp-769317) | 0.3335 | 0.000 | 3 |
Ca4Nb2O9 (mp-31016) | 0.3378 | 0.000 | 3 |
TiCdO3 (mp-20940) | 0.3435 | 0.040 | 3 |
LaMnO3 (mp-629046) | 0.3360 | 0.120 | 3 |
Ca3Nb2CoO9 (mp-640228) | 0.2910 | 0.000 | 4 |
Ca2MnSbO6 (mvc-11569) | 0.2992 | 0.016 | 4 |
PrMgV2O6 (mvc-9384) | 0.3100 | 0.141 | 4 |
Ca3Nb2CoO9 (mvc-16562) | 0.2877 | 0.000 | 4 |
CaHoV2O6 (mvc-10337) | 0.2835 | 0.044 | 4 |
Ca5Gd3Ti5Mn3O24 (mp-744410) | 0.0992 | 0.013 | 5 |
Ca5Y3Ti5Mn3O24 (mp-743716) | 0.0497 | 0.156 | 5 |
Ca5Dy3Ti5Mn3O24 (mp-743698) | 0.0483 | 0.020 | 5 |
CaSmMnSnO6 (mp-698702) | 0.2810 | 0.177 | 5 |
Ca16Zr9Ta7N7O41 (mp-677269) | 0.2623 | 0.046 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Ca_sv Ho_3 Ti_pv Mn_pv O |
Final Energy/Atom-7.9135 eV |
Corrected Energy-338.4369 eV
-338.4369 eV = -316.5394 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)