Final Magnetic Moment5.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.004 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2Mn2(SO4)3 + K2SO4 + H2O |
Band Gap3.902 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 206.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 -1> | 224.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 231.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 323.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 231.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 308.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 231.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 231.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 275.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 231.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 231.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 231.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 154.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 222.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 138.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 323.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 275.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 224.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 222.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 231.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 275.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 245.1 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 231.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 231.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 231.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 308.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 323.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 323.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 231.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 231.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 184.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 206.7 |
BN (mp-984) | <1 0 0> | <1 1 0> | 174.8 |
BN (mp-984) | <1 0 1> | <1 1 0> | 262.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 231.0 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 308.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 245.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 231.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 277.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 231.0 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 231.0 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 231.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 295.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 231.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 262.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 -1> | 224.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 0> | 262.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InTeI7 (mp-680058) | 0.7182 | 0.000 | 3 |
GaTeI7 (mp-29541) | 0.7499 | 0.000 | 3 |
FeH4(SO5)2 (mp-772432) | 0.5670 | 0.059 | 4 |
Fe3P2(HO)16 (mp-742859) | 0.5800 | 0.018 | 4 |
Hg3H4S2O11 (mp-721053) | 0.5884 | 0.003 | 4 |
ZnH8SO8 (mp-24708) | 0.5965 | 0.016 | 4 |
Mn5P4(HO2)10 (mp-744430) | 0.5998 | 0.003 | 4 |
Li2NiH12(SO7)2 (mp-771658) | 0.5390 | 0.045 | 5 |
Li2FeH12(SO7)2 (mp-770572) | 0.4938 | 0.064 | 5 |
K2FeH4(SO5)2 (mp-644324) | 0.5364 | 0.005 | 5 |
Rb2Cr2Cd(H2O5)2 (mp-566668) | 0.4276 | 0.000 | 5 |
K2FeH4(SO5)2 (mp-743846) | 0.1441 | 0.003 | 5 |
NaMnP2H10NO10 (mp-761339) | 0.7240 | 0.017 | 6 |
RbScBP2HO9 (mp-23809) | 0.7216 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: K_sv Mn_pv H S O |
Final Energy/Atom-5.7966 eV |
Corrected Energy-240.3316 eV
-240.3316 eV = -220.2703 eV (uncorrected energy) - 16.6996 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)