Final Magnetic Moment5.196 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.892 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.208 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg3Si4(HO6)2 + Mg2SiO4 + Mg45Si32(H29O69)2 + Fe2O3 |
Band Gap1.652 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 291.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 291.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 291.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 291.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 333.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 333.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 251.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 166.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 333.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 333.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 208.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 208.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 166.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 333.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 250.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 173.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 251.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 333.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 166.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 333.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 291.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 333.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 208.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 208.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 166.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 291.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 208.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 291.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 166.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 291.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 208.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 250.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 291.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 208.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 333.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 291.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 291.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 333.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 166.7 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 333.4 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 208.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 250.0 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 173.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 208.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 333.4 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 166.7 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 208.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 250.0 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 166.7 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 125.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg16Si7HO32 (mp-707534) | 0.6567 | 0.174 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Mg_pv Fe_pv Si H O |
Final Energy/Atom-6.6323 eV |
Corrected Energy-600.1908 eV
-600.1908 eV = -563.7478 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 2.7330 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)