Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.812 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.803 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.7 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 157.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 216.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 157.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 289.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 216.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 139.7 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 208.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 188.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.7 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 253.8 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 104.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 139.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 208.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 139.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 216.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 289.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 289.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 144.6 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 104.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 72.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 289.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 216.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 139.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 144.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 72.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 208.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 289.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 289.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 1> | 188.8 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 216.9 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 104.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 139.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 289.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 1> | 188.8 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 1> | 157.3 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 289.3 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 208.6 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 1> | 157.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 208.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 289.3 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 216.9 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 216.9 |
C (mp-48) | <0 0 1> | <0 1 1> | 126.9 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 144.6 |
WSe2 (mp-1821) | <1 1 0> | <0 1 1> | 253.8 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 139.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 289.3 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 1> | 253.8 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 139.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na6Mo11O36 (mp-642881) | 0.6946 | 0.005 | 3 |
Mn2O2F9 (mp-504690) | 0.6949 | 0.000 | 3 |
Te(HO)6 (mp-625941) | 0.7205 | 0.089 | 3 |
TeHO3 (mp-625657) | 0.6329 | 0.027 | 3 |
YFe3F15 (mvc-6574) | 0.7185 | 0.456 | 3 |
ZrSCl6O (mp-554265) | 0.7439 | 0.000 | 4 |
HgTe(H2O3)2 (mp-605347) | 0.7041 | 0.040 | 4 |
LiVWO6 (mp-768026) | 0.7423 | 0.054 | 4 |
Ba2AlV2F11 (mvc-9685) | 0.7294 | 0.044 | 4 |
Ba2AlFe2F11 (mvc-9732) | 0.7128 | 0.027 | 4 |
V2F7 (mp-765242) | 0.6832 | 0.089 | 2 |
Rb2FeH2Cl5O (mp-735545) | 0.3007 | 0.159 | 5 |
K2InH2Cl5O (mp-766966) | 0.4091 | 0.000 | 5 |
H2RhN2Cl5O (mp-706921) | 0.3546 | 0.929 | 5 |
K2FeH2Cl5O (mp-25745) | 0.3434 | 0.000 | 5 |
K2CrH2Cl5O (mp-542691) | 0.3914 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Rb_sv Cr_pv H Cl O |
Final Energy/Atom-4.2301 eV |
Corrected Energy-196.9848 eV
-196.9848 eV = -186.1237 eV (uncorrected energy) - 8.0520 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)